Friction and Wear of Hard Yet Tough TiN Coatings Deposited Using High-Power Impulse Magnetron Sputtering

Qian Zhou, Yixiang Ou, Feiqiang Li, Changyu Ou, Wenbin Xue, Bin Liao, Qingsong Hua, Yunfei Xu, Jidong Cao, Guanshu Qu

Coatings · 10.05.2024 · 14 (5) · 598

DOI: 10.3390/coatings14050598 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Coatings, online erschienen am 10.05.2024. Verfasst von Qian Zhou und 9 weiteren Autor:innen. Die Arbeit wurde bisher 11-mal zitiert (Crossref) und nennt 34 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, 2024 innovation projects from Beijing Academy of Science and Technology, the Guangdong Province Key Area Research and Development Program, National Key R&D Program of China.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The friction and wear response of hard coatings is complex, which largely depends on a good combination of hardness and toughness, and their service life is difficult to predict. Hence, in this work, hard yet tough TiN coatings were deposited using high-power impulse magnetron sputtering at 5–10 kW. With increasing sputtering power, the coatings showed a transition in crystal texture from (200) to (111), along with a refinement in microstructure, leading to an improvement in hardness (H) of 29.8–31.2 GPa and an effective Young’s modulus (E*) of 310–365 GPa. The hard yet tough TiN coatings deposited at 6.5 kW exhibited the highest H/E* and H3/E*2 ratios of 0.097 and 0.29, respectively, as well as the highest fracture toughness of 2.1 MPa·m1/2 and elastic recovery of 42.5%. Accordingly, the coatings possessed an enhanced adhesion and cohesion, in terms of micro-scratch critical load (LC3 = 19.67 N) and HF Rockwell HF1 level. The friction and wear response of hard yet tough TiN coatings under the normal load of 1–10 N were investigated to explore their durability and predict their critical load up to failure. Wear mechanisms changed from oxidative to severe abrasive wear, with load increasing from 1 to 10 N. At 2–5 N, a combination of oxidative and abrasive wear was observed. The coatings maintained their integrity up to the critical load of 9.4 N before failure event, with a maximum wear track depth of 1.8 μm, indicating their durability under the loading conditions.

Förderung

  • National Natural Science Foundation of China
  • 2024 innovation projects from Beijing Academy of Science and Technology, the Guangdong Province Key Area Research and Development Program
  • National Key R&D Program of China

Zitieren

APA

Zhou, Q., Ou, Y., Li, F., Ou, C., Xue, W., Liao, B., Hua, Q., Xu, Y., Cao, J., & Qu, G. (2024). Friction and Wear of Hard Yet Tough TiN Coatings Deposited Using High-Power Impulse Magnetron Sputtering. Coatings, 14(5), 598. https://doi.org/10.3390/coatings14050598

Vancouver

Zhou Q, Ou Y, Li F, Ou C, Xue W, Liao B, et al. Friction and Wear of Hard Yet Tough TiN Coatings Deposited Using High-Power Impulse Magnetron Sputtering. Coatings. 2024;14(5):598. doi:10.3390/coatings14050598

BibTeX
@article{Zhou2024,
  author = {Zhou, Qian and Ou, Yixiang and Li, Feiqiang and Ou, Changyu and Xue, Wenbin and Liao, Bin and Hua, Qingsong and Xu, Yunfei and Cao, Jidong and Qu, Guanshu},
  title = {Friction and Wear of Hard Yet Tough TiN Coatings Deposited Using High-Power Impulse Magnetron Sputtering},
  journal = {Coatings},
  year = {2024},
  volume = {14},
  number = {5},
  pages = {598},
  doi = {10.3390/coatings14050598}
}
Kostenlos starten →