Comparison of the Mechanical Properties and Corrosion Resistance of the Cr-CrN, Ti-TiN, Zr-ZrN, and Mo-MoN Coatings

He Tao, Valery Zhylinski, Alexey Vereschaka, Vadzim Chayeuski, Huo Yuanming, Filipp Milovich, Catherine Sotova, Anton Seleznev, Olga Salychits

Coatings · 08.04.2023 · 13 (4) · 750

DOI: 10.3390/coatings13040750 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Coatings, online erschienen am 08.04.2023. Verfasst von He Tao und 8 weiteren Autor:innen. Die Arbeit wurde bisher 39-mal zitiert (Crossref) und nennt 94 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Natural Science Foundation of Shanghai, International cooperative scientific research platform of SUES.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

In this work, the mechanical properties and corrosion resistance of Cr-CrN, Ti-TiN, Zr-ZrN, and Mo-MoN coatings deposited by the physical vapor deposition (PVD) method on Ti-6Al-4V alloy were compared. The phase composition of the coatings, their hardness and fracture resistance in scratch tests were determined, and their structural characteristics were also studied using a scanning electron microscope (SEM) and a transmission electron microscope (TEM). The diffraction spectra were made using an automatic X-ray diffractometer. The value of the adhesive component of the friction coefficient fadh of the pair “coated and uncoated Ti-6Al-4V alloy” was investigated in the temperature range of 20–900 °C. The lowest value of fadh was detected for the Zr-ZrN coating at temperatures below 400 °C, while for the Mo-MoN coating it was observed at temperatures above 700 °C. The polarization curves of the coated and uncoated samples were performed in a 3% aqueous NaCl solution. The level of corrosion of the Ti-6Al-4V alloy samples with Cr-CrN, Ti-TiN, Zr-ZrN, and Mo-MoN coatings was evaluated using the Tafel extrapolation method, the iteration method, and the polarization resistance method. The results obtained with these methods indicate that the Zr-ZrN coated sample has the best corrosion resistance in the 3 wt.% NaCl solution, with a corrosion current density of 0.123 μA/cm2.

Förderung

  • National Natural Science Foundation of China
  • Natural Science Foundation of Shanghai
  • International cooperative scientific research platform of SUES

Zitieren

APA

Tao, H., Zhylinski, V., Vereschaka, A., Chayeuski, V., Yuanming, H., Milovich, F., Sotova, C., Seleznev, A., & Salychits, O. (2023). Comparison of the Mechanical Properties and Corrosion Resistance of the Cr-CrN, Ti-TiN, Zr-ZrN, and Mo-MoN Coatings. Coatings, 13(4), 750. https://doi.org/10.3390/coatings13040750

Vancouver

Tao H, Zhylinski V, Vereschaka A, Chayeuski V, Yuanming H, Milovich F, et al. Comparison of the Mechanical Properties and Corrosion Resistance of the Cr-CrN, Ti-TiN, Zr-ZrN, and Mo-MoN Coatings. Coatings. 2023;13(4):750. doi:10.3390/coatings13040750

BibTeX
@article{Tao2023,
  author = {Tao, He and Zhylinski, Valery and Vereschaka, Alexey and Chayeuski, Vadzim and Yuanming, Huo and Milovich, Filipp and Sotova, Catherine and Seleznev, Anton and Salychits, Olga},
  title = {Comparison of the Mechanical Properties and Corrosion Resistance of the Cr-CrN, Ti-TiN, Zr-ZrN, and Mo-MoN Coatings},
  journal = {Coatings},
  year = {2023},
  volume = {13},
  number = {4},
  pages = {750},
  doi = {10.3390/coatings13040750}
}
Kostenlos starten →