Corrosion Failure Analysis of a Reducing Tee at a Shale Gas Station

Lincai Peng, Shaomu Wen, Xiaochun Zheng, Ying Xiong, Xueke Chen, Ting Mao, Hongjie Li

Corrosion and Materials Degradation · 2026-10-29 · 7 (4) · 71

DOI: 10.3390/cmd7040071 ↗

At a glance

Journal article in Corrosion and Materials Degradation, published online on 2026-10-29. Written by Lincai Peng and 6 co-authors. 36 references. The full text is freely available (open access, CC BY 4.0). Funded by: Science and Technology Major Project of PetroChina.

AbstraktBibliografické údajeCiteRelated studies

Abstract (original language)

To investigate the corrosion failure of a reducing tee at a shale gas station, a failure analysis was carried out. The failed tee was made of L245N steel, with a large-diameter branch of DN 80 and a small-diameter branch of DN 25. The DN 80 branch conveyed shale gas, while the DN 25 branch served as a vent and remained closed. The tee was after approximately 20 months of service. By means of macroscopic observation, transported medium analysis, chemical composition testing of the pipe fitting, hardness testing, metallographic structure examination, and analysis of the composition and morphology of corrosion products, the corrosion failure mechanism was identified. The chemical composition and mechanical properties of the tee met the standard requirements, the inclusion content was low, and the microstructure was normal. A substantial quantity of loose, lamellar and block-like corrosion products had formed at and around the perforation. The corrosion pit regions were mainly composed of Fe, C, O, and a small amount of S. The corroded areas exhibited pitting, ring-like corrosion, and mesa attack. The corrosion products were predominantly FeCO3, with a small amount of FeS. Comprehensive analysis indicates that the synergistic corrosion effect of carbon dioxide (CO2) and sulfate-reducing bacteria (SRB) is the root cause of the corrosion perforation of the tee.

Funding

  • Science and Technology Major Project of PetroChina

Cite

APA

Peng, L., Wen, S., Zheng, X., Xiong, Y., Chen, X., Mao, T., & Li, H. (2026). Corrosion Failure Analysis of a Reducing Tee at a Shale Gas Station. Corrosion and Materials Degradation, 7(4), 71. https://doi.org/10.3390/cmd7040071

Vancouver

Peng L, Wen S, Zheng X, Xiong Y, Chen X, Mao T, et al. Corrosion Failure Analysis of a Reducing Tee at a Shale Gas Station. Corrosion and Materials Degradation. 2026;7(4):71. doi:10.3390/cmd7040071

BibTeX
@article{Peng2026,
  author = {Peng, Lincai and Wen, Shaomu and Zheng, Xiaochun and Xiong, Ying and Chen, Xueke and Mao, Ting and Li, Hongjie},
  title = {Corrosion Failure Analysis of a Reducing Tee at a Shale Gas Station},
  journal = {Corrosion and Materials Degradation},
  year = {2026},
  volume = {7},
  number = {4},
  pages = {71},
  doi = {10.3390/cmd7040071}
}
Start for free →