A Post-Processing Framework for Crack–Hole Interaction: Amplification, Deflection, and Capture Across Eight Geometries

Abdulnaser M. Alshoaibi, Yahya Ali Fageehi

Applied Sciences · 20.11.2026 · 16 (22) · 11520

DOI: 10.3390/app162211520 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Applied Sciences, online erschienen am 20.11.2026. Verfasst von Abdulnaser M. Alshoaibi und 1 weiteren Autor:innen. Die Arbeit nennt 40 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Deanship of Graduate Studies and Scientific Research at Jazan University.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Holes are widely proposed as crack arrestors, but crack-growth simulations usually report the crack path without defining arrest in a linear-elastic model or explaining its mechanism. This paper proposes a post-processing framework for crack–hole interaction and applies it to previously reported ANSYS SMART simulations of eight hole-bearing geometries. The framework combines a matched-pair hole amplification factor Λ (the mode-I stress-intensity ratio with and without holes at equal crack extension), a steering angle reconstructed from KI and KII, a three-regime classification (capture, deflection and escape, hole switching), and a distinction between geometric and mechanical arrest. In the three-point-bending beam the perforated crack ends at the middle hole although KI is 1.6–2.1 times that of the hole-free beam, so termination reflects capture, not relief; the four-point-bending specimen gives Λ ≈ 1.1–1.5. Handbook-based estimates for the modified CT specimens and the one-hole plate also exceed 1, but the source data for these cases are inconsistent, so the estimates are indicative only and are not counted as evidence. A persistent sign of KII identifies the capturing hole in the notched plate and CT specimens, and a 0.8 mm shift in the pre-crack changes the hole captured; this sensitivity comes from single runs and has not yet been checked for numerical convergence. A reporting protocol specifies the further runs needed, including convergence checks of the crack path and a hole-free twin of the modified CT specimen. The conclusions rest on signs, trends and ratios and are testable hypotheses, not a universal arrest criterion.

Förderung

  • Deanship of Graduate Studies and Scientific Research at Jazan University

Zitieren

APA

Alshoaibi, A. M., & Fageehi, Y. A. (2026). A Post-Processing Framework for Crack–Hole Interaction: Amplification, Deflection, and Capture Across Eight Geometries. Applied Sciences, 16(22), 11520. https://doi.org/10.3390/app162211520

Vancouver

Alshoaibi AM, Fageehi YA. A Post-Processing Framework for Crack–Hole Interaction: Amplification, Deflection, and Capture Across Eight Geometries. Applied Sciences. 2026;16(22):11520. doi:10.3390/app162211520

BibTeX
@article{Alshoaibi2026,
  author = {Alshoaibi, Abdulnaser M. and Fageehi, Yahya Ali},
  title = {A Post-Processing Framework for Crack–Hole Interaction: Amplification, Deflection, and Capture Across Eight Geometries},
  journal = {Applied Sciences},
  year = {2026},
  volume = {16},
  number = {22},
  pages = {11520},
  doi = {10.3390/app162211520}
}
Kostenlos starten →