Abstract (Originalsprache)
In this study, a GH3536 coating was fabricated on a GH3536 substrate via laser cladding. Response surface methodology was applied to investigate the influences of process parameters on cladding layer characteristic dimensions, and statistical regression models were built for predicting single-track geometrical morphologies. The results reveal that laser power, scanning speed, and powder feeding rate jointly govern cladding layer morphology. The clad width increases with rising laser power, whereas it decreases with increasing scanning speed and powder feeding rate. The clad height increases with higher powder feeding rate and decreases with higher scanning speed. The clad depth decreases with higher powder feeding rate and increases with higher laser power. Both the aspect ratio and dilution rate increase with laser power and scanning speed, while decreasing with higher powder feeding rate. The optimized process parameters are determined as 600 W laser power, 4 mm/s scanning speed, and 0.6 r/min powder feeding rate. The as-deposited coating contains equiaxed and columnar dendrites, and obvious recrystallization emerges after solution heat treatment. Cavitation-erosion tests indicate that the solution heat treatment can significantly improve the cavitation-erosion resistance of GH3536 alloy. After 10 h cavitation erosion, the average erosion rates of the as-deposited, forged, and solution heat-treated alloys are 1.15, 0.29, and 0.17 mg/(cm2 h), respectively. The cavitation-erosion resistance ranks in the descending order: solution heat-treated, forged, and as-deposited. Heat treatment homogenizes and stabilizes the microstructure, thereby inhibiting the initiation and propagation of cavitation damage and significantly enhancing the cavitation-erosion resistance of the GH3536 alloy.
Förderung
- Education department of zhejiang province
- Zhejiang institute of economics and trade
Zitieren
APA
Xu, B., Chen, L., Zheng, X., Zhang, Y., Xiang, F., & Yang, Y. (2026). Process optimization and cavitation resistance behavior of GH3536 alloy fabricated via laser cladding. Journal of Laser Applications, 38(4). https://doi.org/10.2351/7.0002110
Vancouver
Xu B, Chen L, Zheng X, Zhang Y, Xiang F, Yang Y. Process optimization and cavitation resistance behavior of GH3536 alloy fabricated via laser cladding. Journal of Laser Applications. 2026;38(4). doi:10.2351/7.0002110
BibTeX
@article{Xu2026,
author = {Xu, Bing and Chen, Liangliang and Zheng, Xueqing and Zhang, Yu and Xiang, Fangyi and Yang, Ying},
title = {Process optimization and cavitation resistance behavior of GH3536 alloy fabricated via laser cladding},
journal = {Journal of Laser Applications},
year = {2026},
volume = {38},
number = {4},
doi = {10.2351/7.0002110}
}
EUVIMED