Effects of Light Curing on the Mechanical Properties and Shade Stability of a Dual-Cure Bulk-Fill Resin Composite

H Alzraikat, G A Maghaireh, A Alomari, R B Price

Operative Dentistry · 2026-03 · 51 (2) · 167-179

DOI: 10.2341/25-131-l ↗

Kurz gefasst

Fachartikel in der Zeitschrift Operative Dentistry, 2026-03. Verfasst von H Alzraikat und 3 weiteren Autor:innen. Hauptthemen laut MEDLINE: Composite Resins, Dental Restoration, Permanent, Curing Lights, Dental. Die Arbeit nennt 48 Literaturangaben.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Rationale

Despite the growing use of dual-cure bulk-fill resin composites (RCs), the influence of light-curing protocols on their polymerization and material behavior remains unclear. Understanding these effects is critical for optimizing clinical outcomes.

Objective

This study investigated degree of conversion, flexural strength, flexural modulus, water sorption and solubility, and shade stability of a dual-cure bulk-fill RC, Bulk-EZ Plus (BZ), compared to a light-cured bulk-fill RC, Filtek-One Bulk-Fill (FB).

Methods

Specimens were randomized into five groups: BZ self-cured (BZ-SC), BZ light-cured for 10-seconds (BZ-10), BZ light-cured for 20-seconds (BZ-20), FB light-cured for 20-seconds (FB-20), and FB light-cured for 40 seconds (FB-40). Degree of conversion was evaluated using FTIR spectroscopy, flexural strength and modulus, and water sorption and solubility were determined following ISO 4049:2019. Shade stability in coffee and distilled water was measured using a spectrophotometer after 24 hours, seven days, and 21 days. Two-way ANOVA assessed the effects of RC type and curing protocol. Shade stability was analyzed using repeated measures and three-way ANOVA (α = 0.05).

Results

Light activation increased the flexural modulus of BZ ( p = 0.012 and p = 0.001 for BZ-SC vs. BZ-10 and BZ-20, respectively) and flexural strength ( p = 0.018 for BZ-SC vs BZ-20), and reduced water sorption (both p < 0.001) and solubility ( p = 0.028 for BZ-SC vs. BZ-10 and p = 0.001 for BZ-SC vs BZ-20). Extending light exposure from 20 seconds to 40 seconds did not change the flexural strength and modulus, or water sorption and solubility of FB (all p > 0.05).

Conclusion

Light activation improved the physical and mechanical properties of the dual-cure bulk-fill resin composite (Bulk-EZ Plus), but increasing the light exposure time did not improve the properties of the light-cured bulk-fill material (Filtek-One Bulk-Fill).

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

Composite ResinsDental Restoration, PermanentCuring Lights, DentalLightPolymerizationFlexural Strength

Substanzen

Composite Resins

Zitieren

APA

Alzraikat, H., Maghaireh, G. A., Alomari, A., & Price, R. B. (2026). Effects of Light Curing on the Mechanical Properties and Shade Stability of a Dual-Cure Bulk-Fill Resin Composite. Operative Dentistry, 51(2), 167-179. https://doi.org/10.2341/25-131-l

Vancouver

Alzraikat H, Maghaireh GA, Alomari A, Price RB. Effects of Light Curing on the Mechanical Properties and Shade Stability of a Dual-Cure Bulk-Fill Resin Composite. Operative Dentistry. 2026;51(2):167-179. doi:10.2341/25-131-l

BibTeX
@article{Alzraikat2026,
  author = {Alzraikat, H and Maghaireh, G A and Alomari, A and Price, R B},
  title = {Effects of Light Curing on the Mechanical Properties and Shade Stability of a Dual-Cure Bulk-Fill Resin Composite},
  journal = {Operative Dentistry},
  year = {2026},
  volume = {51},
  number = {2},
  pages = {167--179},
  doi = {10.2341/25-131-l}
}
Kostenlos starten →