Abstract (Originalsprache)
The abrasion resistance of martensitic iron alloys used for cast machine components operating under abrasive wear conditions can be improved by producing carbides of elements such as V, W, and Mo in the alloy matrix. The aim of the conducted research was to evaluate the effect of the addition of carbide-forming elements such as V, W, and Mo on the microstructure and abrasion resistance determined in the Miller test. During the metallurgical process, carbide-forming elements such as vanadium and tungsten were introduced into the tested alloys at 12.7 and 10.6 wt.%, and at 3.3 and 2.6 wt.%, respectively, with a total carbon content of 4.0 and 4.3 wt.%. An additional 0.006% by weight of boron was added to one of the alloys.. The effect of boron microaddition on the hardenability and microstructural evolution of high-carbon Fe-C-V-W-Mo casting alloys containing a large fraction of carbide-forming elements remains insufficiently understood. The measured hardness of the tested samples was from 458 ±9 to 552 ±16 HV in the as-cast condition. This value increased to 875 ±19 HV after hardening, and the highest hardness of 923 ±11 HV was obtained for the alloy M2, which contained 0.006 wt.% B. The microstructure of the tested samples was composed of a martensitic matrix with traces of retained austenite and rod-shaped carbides with a spherical cross-section, which were identified as complex (V,W)xCy carbides. The highest abrasive wear resistance was obtained for the martensitic alloy with 10.6 wt.% V+2.6 wt.% W+0.006 wt.% B, quenched from 880°C and cooled in 15% HI polymer. Its hardness was 923 ±11 HV, and the mass loss was three times lower than that of the reference cast GX70CrMnSiNiMo2 steel.
Zitieren
APA
Tęcza, G. (2026). Microstructure and abrasion resistance of martensitic Fe-C-V-W-Mo casting alloys with and without boron microaddition. Journal of Mining and Metallurgy, Section B: Metallurgy, 26-26. https://doi.org/10.2298/jmmb251120026t
Vancouver
Tęcza G. Microstructure and abrasion resistance of martensitic Fe-C-V-W-Mo casting alloys with and without boron microaddition. Journal of Mining and Metallurgy, Section B: Metallurgy. 2026:26-26. doi:10.2298/jmmb251120026t
BibTeX
@article{Tcza2026,
author = {Tęcza, Grzegorz},
title = {Microstructure and abrasion resistance of martensitic Fe-C-V-W-Mo casting alloys with and without boron microaddition},
journal = {Journal of Mining and Metallurgy, Section B: Metallurgy},
year = {2026},
number = {00},
pages = {26--26},
doi = {10.2298/jmmb251120026t}
}
EUVIMED