Abstract (Originalsprache)

Introduction

Debondable and repairable epoxy-based vitrimer adhesives offer a sustainable solution to conventional epoxy adhesives for structural applications. This study evaluated the performance of a vitrimer adhesive in structural single-lap-bonded joints and investigated its repairability and debonding characteristics in comparison with those of a conventional epoxy adhesive. Materials and methods: Metal substrates, aluminum (Al6061) and stainless steel (SS303), were used to fabricate similar and dissimilar single-lap-bonded joints with vitrimer and conventional epoxy adhesives. Lap shear strength (LSS) testing was conducted to evaluate the mechanical performance. The debonding behavior was examined using a mixed solvent system of dimethylformamide (DMF) and ethylene glycol (EG) at different temperatures. Repairability was evaluated through repeated repair cycles, and the retained properties were investigated.

Results

Results revealed that the vitrimer-bonded joints exhibited a maximum lap shear strength of 8.8 MPa. A mixed cohesive–adhesive failure mode was observed in the vitrimer-bonded joints for both similar and dissimilar substrate-bonded joints. The repaired vitrimer adhesive-bonded joints retained 89%, 82%, and 67% of their original lap shear strength after the first, second, and third repair cycles, respectively. Elevated temperatures significantly accelerated the debonding process, with complete debonding achieved within 90 min at 150 °C, whereas debonding required 5–6 h at 80 °C and approximately 36 h under ambient conditions.

Conclusions

The results demonstrate the successful repair of vitrimer adhesive-bonded joints up to the second cycle with 82% retained properties, and easy debonding makes them a promising candidate for applications in sustainable structural adhesives.

Zitieren

APA

Nartam, S., Budhe, S., Paul, J., & Barros, S. D. (2026). Strength, repairability, and debonding of vitrimer structural adhesive joints. Academia Materials Science, 3(2). https://doi.org/10.20935/acadmatsci8358

Vancouver

Nartam S, Budhe S, Paul J, Barros SD. Strength, repairability, and debonding of vitrimer structural adhesive joints. Academia Materials Science. 2026;3(2). doi:10.20935/acadmatsci8358

BibTeX
@article{Nartam2026,
  author = {Nartam, Sudhanshu and Budhe, Sandip and Paul, Jinu and Barros, Silvio de},
  title = {Strength, repairability, and debonding of vitrimer structural adhesive joints},
  journal = {Academia Materials Science},
  year = {2026},
  volume = {3},
  number = {2},
  doi = {10.20935/acadmatsci8358}
}
Kostenlos starten →