EUVIMEDEUVIMED entdecken
Crossref

Comparative Evaluation of Flexural Strength of Glass Ionomer Cement and Cention N in Artificial Medium Over Time Intervals - An In-Vitro Study

Risana K., Prathyusha P, Amith Adyanthaya, Aparna Sivaraman, Nazreen Ayub K, Reshma Aloysius, Sangeetha C.R, Swetha S. Nair

Journal of Evolution of Medical and Dental Sciences · 09.08.2021 · 10 (32) · 2609-2614

DOI: 10.14260/jemds/2021/534 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Evolution of Medical and Dental Sciences, online erschienen am 09.08.2021. Verfasst von Risana K. und 7 weiteren Autor:innen. Die Arbeit wurde bisher 4-mal zitiert (Crossref) und nennt 22 Literaturangaben.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

BACKGROUND Glass ionomer cement (GIC) is a versatile restorative cement in paediatric dentistry. Due to its less flexural strength, alternative materials have been developed. Cention N is one such material, but since it’s a new material evidence is lacking regarding its physical properties, especially flexural strength for evaluating its clinical outcome. We wanted to compare the flexural strength of glass ionomer cement and Cention N stored in artificial saliva and its variation over different time intervals, i.e., after 24 hours, 1 week and 4 weeks. METHODS A total of 30 specimens were prepared for GIC (Fuji IX) and Cention N and were further categorized according to the duration of storage time of 24 hours, 1 week and 4 weeks (N = 10). A 3 - point bending test using a universal testing machine was used to evaluate the flexural strength. RESULTS GIC Fuji IX showed a mean flexural strength of 35.296 ± 1.61 Mpa at the end of 24 hours, 47.234 ± 4.12 after 1 week and 66.039 ± 11.05 Mpa at the end of 4 weeks. GIC showed a statistically significant increase of flexural strength from 24 hours to one week and a further increase after 4 weeks of storage. The flexural strength of Cention N at 24 hours was 175.985 ± 22.11 Mpa, at the end of one week was 163.486 ± 17.55 MPa, and after 4 weeks was 175.437 ± 27.22 Mpa. Cention N did not show any statistically significant change in flexural strength value from 24 hours to 4 weeks. Cention N showed highly significant difference between flexural strength compared to GIC at all - time intervals. CONCLUSIONS Cention N has a superior flexural strength compared to GIC at all - time intervals. KEY WORDS Cention N, Flexural Strength, Glass Ionomer Cement

Zitieren

APA

K., R., P, P., Adyanthaya, A., Sivaraman, A., K, N. A., Aloysius, R., C.R, S., & Nair, S. S. (2021). Comparative Evaluation of Flexural Strength of Glass Ionomer Cement and Cention N in Artificial Medium Over Time Intervals - An In-Vitro Study. Journal of Evolution of Medical and Dental Sciences, 10(32), 2609-2614. https://doi.org/10.14260/jemds/2021/534

Vancouver

K. R, P P, Adyanthaya A, Sivaraman A, K NA, Aloysius R, et al. Comparative Evaluation of Flexural Strength of Glass Ionomer Cement and Cention N in Artificial Medium Over Time Intervals - An In-Vitro Study. Journal of Evolution of Medical and Dental Sciences. 2021;10(32):2609-2614. doi:10.14260/jemds/2021/534

BibTeX
@article{K2021,
  author = {K., Risana and P, Prathyusha and Adyanthaya, Amith and Sivaraman, Aparna and K, Nazreen Ayub and Aloysius, Reshma and C.R, Sangeetha and Nair, Swetha S.},
  title = {Comparative Evaluation of Flexural Strength of Glass Ionomer Cement and Cention N in Artificial Medium Over Time Intervals - An In-Vitro Study},
  journal = {Journal of Evolution of Medical and Dental Sciences},
  year = {2021},
  volume = {10},
  number = {32},
  pages = {2609--2614},
  doi = {10.14260/jemds/2021/534}
}
Kostenlos starten →