Study on the mechanical behavior and rupture characteristics of coal after thermal damage
PLOS ONE · 2024
DOI: 10.1371/journal.pone.0315468 ↗Kurz gefasst
Fachartikel in der Zeitschrift PLOS ONE, 2024. Verfasst von Chuan Li und 4 weiteren Autor:innen. Beteiligte Einrichtung: College of Mining, Guizhou University, Guiyang, PR China. Hauptthemen laut MEDLINE: Coal, Hot Temperature. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 48 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Guizhou Provincial Science and Technology Plan Project, National Natural Science Foundation of China, Guizhou Provincial of Social Funding Project.
Abstract (Originalsprache)
High temperature is a critical safety concern that poses challenges to the safe and efficient operation of coal mines. To explore the mechanical behavior and fracture mechanisms of coal exposed to high temperatures, coal samples were subjected to various thermal treatments. After cooling, uniaxial compression tests were performed using an electronic universal testing machine to assess their macroscopic properties. A discrete element numerical model, reflecting the same mineral composition, was then developed to investigate the microscopic fracture behavior of thermally treated coal under uniaxial compression. The results indicate that at high temperatures, thermal motion becomes more pronounced, leading to increased particle displacement and a transition in coal failure from brittle to ductile behavior. High temperatures intensify thermal damage, generating numerous thermal cracks, which prolong the crack closure phase and delay the onset of the elastic deformation stage. Furthermore, the formation and propagation of these thermal cracks significantly influence macroscopic mechanical properties. Peak stress and elastic modulus decrease with rising temperature, with the most pronounced reductions occurring between 200°C and 300°C, where the thermal damage factor peaks at 0.72. As the temperature increases, the proportion of tensile cracks decreases, while shear cracks become more prevalent. Under heat treatment, tensile failure dominates, whereas shear failure is predominant during uniaxial compression. These findings provide valuable insights for improving safety protocols in high-temperature coal mining environments.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Substanzen
Autor:innen und Institutionen
- College of Mining, Guizhou University, Guiyang, PR China.
- Guizhou Vocational College of Culture and Tourism, Guiyang, PR China.
- Guizhou Lindong Coal Industry Development Co., Ltd. Longfeng Coal Mine, Jinsha, Guizhou, PR China.
ORCID-Profile: Chuan Li, Yiping Zhang
Förderung
- Guizhou Provincial Science and Technology Plan Project
- National Natural Science Foundation of China
- Guizhou Provincial of Social Funding Project
Zitieren
APA
Li, C., Zhang, Y., Bu, H., Lan, H., & Heng, X. (2024). Study on the mechanical behavior and rupture characteristics of coal after thermal damage. PLOS ONE. https://doi.org/10.1371/journal.pone.0315468
Vancouver
Li C, Zhang Y, Bu H, Lan H, Heng X. Study on the mechanical behavior and rupture characteristics of coal after thermal damage. PLOS ONE. 2024. doi:10.1371/journal.pone.0315468
BibTeX
@article{Li2024,
author = {Li, Chuan and Zhang, Yiping and Bu, Haijiao and Lan, Hong and Heng, Xianwei},
title = {Study on the mechanical behavior and rupture characteristics of coal after thermal damage},
journal = {PLOS ONE},
year = {2024},
doi = {10.1371/journal.pone.0315468}
}