EUVIMEDAtrasti EUVIMED
Crossref

Effect of Different Concentrations of Nano Hydroxyapatite on the Microshear Bond Strength of Zirconia to Resin Cement

Sakineh Nikzad, Azin Zare, Faezeh Atri, Dana Jafarpour, Shahram Zare, Abbas Azari

The International Journal of Prosthodontics · 2025

DOI: 10.11607/ijp.9205 ↗

At a glance

Journal article in The International Journal of Prosthodontics, 2025. Written by Sakineh Nikzad and 5 co-authors. Major MEDLINE topics: Zirconium, Durapatite, Resin Cements, Dental Bonding.

SantraukaSubjectsBibliografiniai duomenysCiteRelated studies

Abstract (original language)

PURPOSE: To assess the impact of nano-hydroxyapatite (n-HA) coating of different concentrations on the microshear bond strength (µSBS) of zirconia ceramics to resin cements. MATERIALS AND METHODS: A total of 48 Cercon Y-TZP blocks (4 × 4 × 4 mm) were randomly divided into four groups (n = 12): (1) control group, (2) 5-g n-HA coating, (3) 10-g n-HA coating, and (4) 15-g n-HA coating. The specimens were sintered at 1,250°C. The thickness of the coatings was characterized using scanning electron microscopy (SEM). Energy dispersive spectroscopy (EDS) and X-ray diffraction (XRD) analyses were carried out to characterize the surface. All specimens were then bonded to Panavia F2.0 cement. Microshear bond testing was carried out using a universal testing machine. Stereomicroscope imaging was used to evaluate the zirconia surface failure mode. The data were analyzed using Kruskal-Wallis and Mann-Whitney tests, and P < .05 was considered statistically significant. RESULTS: The mean µSBS value of the 5-g n-HA-coated group with a thickness of 7.71± 2.51 µm was 28.30 ± 3.02 MPa, which was significantly higher than the control group with the mean value of 19.94 ± 1.86 MPa (P < .05). The mean µSBS value of the 10-g and 15-g n-HA groups with thicker coatings were 21.66 ± 3.63 MPa and 15.23 ± 3.34 MPa, respectively. Additionally, the main mode of failure for the 5-g n-HA group was a mixed failure. In contrast, the adhesive mode of failure was more dominant in the control group. EDS and XRD analysis revealed the formation of crystalline HA on zirconia blocks, highlighting the predominant zirconia peak at 32 degrees. The SEM analysis of the coated specimens displayed a uniform layer of n-HA coating with evident cracks filled with the resin cement. These cracks themselves can help increase the bond strength between ceramic and resin cement. CONCLUSIONS: A thin coating of nanocrystalline hydroxyapatite on zirconia surfaces can be effective in enhancing the microshear bond strength of these ceramics to resin cements. The microshear bond strength of n-HA-coated zirconia was significantly higher compared to the untreated specimens.

Subjects

MeSH terms (MEDLINE)

ZirconiumDurapatiteResin CementsDental BondingCoated Materials, BiocompatibleMaterials TestingMicroscopy, Electron, ScanningSurface PropertiesX-Ray DiffractionDental Stress AnalysisShear StrengthSpectrometry, X-Ray EmissionYttrium

Substances

ZirconiumDurapatiteResin Cementszirconium oxideCoated Materials, BiocompatibleYttrium

Cite

APA

Nikzad, S., Zare, A., Atri, F., Jafarpour, D., Zare, S., & Azari, A. (2025). Effect of Different Concentrations of Nano Hydroxyapatite on the Microshear Bond Strength of Zirconia to Resin Cement. The International Journal of Prosthodontics. https://doi.org/10.11607/ijp.9205

Vancouver

Nikzad S, Zare A, Atri F, Jafarpour D, Zare S, Azari A. Effect of Different Concentrations of Nano Hydroxyapatite on the Microshear Bond Strength of Zirconia to Resin Cement. The International Journal of Prosthodontics. 2025. doi:10.11607/ijp.9205

BibTeX
@article{Nikzad2025,
  author = {Nikzad, Sakineh and Zare, Azin and Atri, Faezeh and Jafarpour, Dana and Zare, Shahram and Azari, Abbas},
  title = {Effect of Different Concentrations of Nano Hydroxyapatite on the Microshear Bond Strength of Zirconia to Resin Cement},
  journal = {The International Journal of Prosthodontics},
  year = {2025},
  doi = {10.11607/ijp.9205}
}
Start for free →