EUVIMEDAtrasti EUVIMED
Crossref

Evaluation of the Bond Strengths Between Dental Ceramics and Co-Cr Frameworks Made with Digital and Conventional Techniques

Carlo Monaco, Martina Bonvicini, Adolfo Di Fiore, Davide Silvestri, Antonio Arena, Ugo Consolo, Francesca Zicari

The International Journal of Prosthodontics · 2024

DOI: 10.11607/ijp.9055 ↗

At a glance

Journal article in The International Journal of Prosthodontics, 2024. Written by Carlo Monaco and 6 co-authors. Major MEDLINE topics: Dental Bonding, Dental Veneers, Metal Ceramic Alloys, Chromium Alloys.

SantraukaSubjectsBibliografiniai duomenysCiteRelated studies

Abstract (original language)

PURPOSE: To evaluate the influence of different Co-Cr framework manufacturing techniques on the bond strength between metal and two types of veneering ceramics with and without a metal primer. MATERIALS AND METHODS: A total of 72 metal specimens were fabricated using the same Co-Cr alloy (Keramit NP, Nobil Metal) with three different techniques: ingots for casting (Keramit NP); disks for CAD/CAM milling (sinergia diskKeramit NP); and powder for selective laser melting (SLM, Keramit NP-S). Each of the 24-specimen groups was divided into two subgroups, according to the application, or lack thereof, of Nobil Metal Bonding (NMB). Two. different veneering ceramic systems were used: Ceramco iC (Dentsply Sirona) and Noritake Super Porcelain EX-3 (Noritake). The bond strength of the metal-ceramic system was evaluated using the three-point bending test and the modality of failure with SEM analysis. Three-way ANOVA with interactions was used to evaluate the influence of the metal production process, the presence or absence of the bonding agent, and the type of veneering ceramic on ceramic-metal adhesion. RESULTS: All specimens exceeded the minimum bond strength of 25 MPa required by ISO Standard 9693-1:2012. The highest values of adhesion were registered for specimens manufactured with casted metal/Noritake veneering ceramic (40.59 ± 7.30 MPa). The lowest values were registered for specimens manufactured with CAD/CAM metal/NMB/ Ceramco iC veneering ceramic (29.47 ± 3.38 MPa). CONCLUSIONS: The fabrication method and= the type of veneering ceramic had a significant influence on the mean bond strength. The application of the NMB did not show an influence on bond strength.

Subjects

MeSH terms (MEDLINE)

Dental BondingDental VeneersMetal Ceramic AlloysChromium AlloysCeramicsDental PorcelainDental Prosthesis DesignComputer-Aided DesignMaterials TestingDental Stress AnalysisDental Casting TechniqueMicroscopy, Electron, ScanningHumansSurface Properties

Substances

Metal Ceramic AlloysChromium AlloysDental Porcelain

Cite

APA

Monaco, C., Bonvicini, M., Di Fiore, A., Silvestri, D., Arena, A., Consolo, U., & Zicari, F. (2024). Evaluation of the Bond Strengths Between Dental Ceramics and Co-Cr Frameworks Made with Digital and Conventional Techniques. The International Journal of Prosthodontics. https://doi.org/10.11607/ijp.9055

Vancouver

Monaco C, Bonvicini M, Di Fiore A, Silvestri D, Arena A, Consolo U, et al. Evaluation of the Bond Strengths Between Dental Ceramics and Co-Cr Frameworks Made with Digital and Conventional Techniques. The International Journal of Prosthodontics. 2024. doi:10.11607/ijp.9055

BibTeX
@article{Monaco2024,
  author = {Monaco, Carlo and Bonvicini, Martina and Di Fiore, Adolfo and Silvestri, Davide and Arena, Antonio and Consolo, Ugo and Zicari, Francesca},
  title = {Evaluation of the Bond Strengths Between Dental Ceramics and Co-Cr Frameworks Made with Digital and Conventional Techniques},
  journal = {The International Journal of Prosthodontics},
  year = {2024},
  doi = {10.11607/ijp.9055}
}
Start for free →