PURPOSE: To evaluate the fracture-behavior of monolithic crowns made of lithium disilicate (IPS e.max CAD, Ivoclar Vivadent; IniBal LiSi Block, GC Dental) and zirconia-reinforced lithium silicate (Celtra Duo, DeguDent; VITA Zahnfabrik) materials before and after cyclic fatigue aging. MATERIALS AND METHODS: Four groups (n = 22/group) of CAD/CAM fabricated upper incisor crowns were produced. All crowns were luted on metal dies with an adhesive dual-cure resin cement (G-CEM LinkForce, GC Dental). Half of the crowns in each group (n = 11) were statically loaded until fracture, without aging. The remaining crowns were subjected to cyclic fatigue aging for 120,000 cycles (Fmax = 220 N) and then loaded statically until fracture. The fractured models were then visually examined. Scanning electron microsopy (SEM) and energy-dispersive spectroscopy (EDS) were used to evaluate the microstructure of CAD/CAM ceramic materials. The data were statistically analyzed with two-way ANOVA followed by the Tukey HSD test (α = .05). RESULTS: Before cyclic aging, there was no statistically significant difference in load-bearing capacity among the four groups (P = .371). After cyclic aging, load-bearing capacity significantly decreased for all groups (P = .000). While the e.max CAD blocks had significantly higher load-bearing capacity (1061 ± 94 N) than both monolithic ceramic crowns (load-bearing capacities of the groups) (P < .05), no significant difference was obtained with the Initial LiSi Block group (920 ± 140 N) (P = .061). CONCLUSIONS: The mechanical performance of monolithic ceramic crowns fabricated from lithium disilicate was befer than zirconia-reinforced lithium silicate after cyclic fatigue aging. Int J Prosthodont 2023;36:e29-e37.

Subjects

MeSH terms (MEDLINE)

LithiumDental PorcelainCeramicsCrownsSilicatesComputer-Aided DesignMaterials TestingDental Stress AnalysisDental Restoration FailureZirconium

Substances

LithiumDental PorcelainSilicateszirconium oxideZirconium

Cite

APA

Garoushi, S., Säilynoja, E., Vallittu, P. K., & Lassila, L. (2023). Fracture-Behavior of CAD/CAM Ceramic Crowns Before and After Cyclic Fatigue Aging. International Journal of Prosthodontics. https://doi.org/10.11607/ijp.7207

Vancouver

Garoushi S, Säilynoja E, Vallittu PK, Lassila L. Fracture-Behavior of CAD/CAM Ceramic Crowns Before and After Cyclic Fatigue Aging. International Journal of Prosthodontics. 2023. doi:10.11607/ijp.7207

BibTeX
@article{Garoushi2023,
  author = {Garoushi, Sufyan and Säilynoja, Eija and Vallittu, Pekka K and Lassila, Lippo},
  title = {Fracture-Behavior of CAD/CAM Ceramic Crowns Before and After Cyclic Fatigue Aging},
  journal = {International Journal of Prosthodontics},
  year = {2023},
  doi = {10.11607/ijp.7207}
}
Start for free →