EUVIMEDEUVIMED entdecken
VergleichsstudieOpen Access · CC BY 4.0

Comparative Evaluation of Tear Strength of Two Platinum‐Based Maxillofacial Silicone Materials: Siloczest LSR With and Without the Addition of 2.5% Zinc Oxide (ZnO) Nanoparticles and Technovent (m511)—An In Vitro Study

Smitha Sharan iD, D L Sarandha iD, S Sujana iD, Mehul A Shah iD, Vignesh Kamath iD

The Scientific World Journal · 2025

DOI: 10.1155/tswj/3581428 ↗

Kurz gefasst

Vergleichsstudie in der Zeitschrift The Scientific World Journal, 2025. Verfasst von Smitha Sharan und 4 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthodontics Including Crown and Bridge, Dayananda Sagar College of Dental Sciences and Hospital, Bengaluru, India. Hauptthemen laut MEDLINE: Zinc Oxide, Platinum, Nanoparticles, Silicones. Die Arbeit nennt 15 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Objective

The present study aims to evaluate and compare the tear strength of an indigenous platinum‐based maxillofacial silicone material (Siloczest LSR [Liquid Silicone Rubber]) with and without the incorporation of 2%–2.5% zinc oxide nanoparticles, using an imported platinum‐based silicone material (Technovent M511) as the benchmark control. Methodology Sixty‐six unnicked 90° angle specimens (ASTM D624 [American Society for Material and Testing)) were fabricated and divided into three groups: Group A—Siloczest LSR without zinc oxide nanoparticles; Group B—Siloczest LSR with 2.5% zinc oxide nanoparticles; and Group C (control)—Technovent M511. Tear strength was evaluated using a Universal Testing Machine (UTM), and results were statistically analysed to compare the performance of the materials.

Results

Siloczest LSR showed significantly higher tear strength (22.64 N/mm) than Technovent (10.08 N/mm, p < 0.001). The addition of 2.5% ZnO nanoparticles reduced tear strength to 20.54 N/mm ( p < 0.05), indicating no reinforcement benefit.

Conclusion

Siloczest LSR, an indigenous platinum‐based maxillofacial silicone, exhibited higher tear strength than the imported Technovent material, supporting its potential use in clinical prosthetic applications as a cost‐effective maxillofacial material. However, the addition of 2.5% zinc oxide nanoparticles did not improve tear strength and led to a slight reduction. These results highlight the need for further investigation into nanoparticle concentration and dispersion methods to optimize reinforcement without compromising the material’s mechanical integrity and clinical validation.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

Zinc OxidePlatinumNanoparticlesSiliconesMaxillofacial ProsthesisSilicone ElastomersMaterials TestingHumans

Stichwörter der Autor:innen

maxillofacial silicone materialnanoparticlestear strengthzinc oxide

Substanzen

Zinc OxidePlatinumSiliconesSilicone Elastomers

Autor:innen und Institutionen

  • Department of Prosthodontics Including Crown and Bridge, Dayananda Sagar College of Dental Sciences and Hospital, Bengaluru, India.
  • Department of Public Health Dentistry, Government Dental College and Hospital, Jamnagar, Gujarat, India.
  • Department of Prosthodontics Crown and Bridge, Manipal College of Dental Sciences Mangalore, Manipal Academy of Higher Education, Manipal, Karnataka, India.

ORCID-Profile: Smitha Sharan, D L Sarandha, S Sujana, Mehul A Shah, Vignesh Kamath

Zitieren

APA

Sharan, S., Sarandha, D. L., Sujana, S., Shah, M. A., & Kamath, V. (2025). Comparative Evaluation of Tear Strength of Two Platinum‐Based Maxillofacial Silicone Materials: Siloczest LSR With and Without the Addition of 2.5% Zinc Oxide (ZnO) Nanoparticles and Technovent (m511)—An In Vitro Study. The Scientific World Journal. https://doi.org/10.1155/tswj/3581428

Vancouver

Sharan S, Sarandha DL, Sujana S, Shah MA, Kamath V. Comparative Evaluation of Tear Strength of Two Platinum‐Based Maxillofacial Silicone Materials: Siloczest LSR With and Without the Addition of 2.5% Zinc Oxide (ZnO) Nanoparticles and Technovent (m511)—An In Vitro Study. The Scientific World Journal. 2025. doi:10.1155/tswj/3581428

BibTeX
@article{Sharan2025,
  author = {Sharan, Smitha and Sarandha, D L and Sujana, S and Shah, Mehul A and Kamath, Vignesh},
  title = {Comparative Evaluation of Tear Strength of Two Platinum‐Based Maxillofacial Silicone Materials: Siloczest LSR With and Without the Addition of 2.5% Zinc Oxide (ZnO) Nanoparticles and Technovent (m511)—An In Vitro Study},
  journal = {The Scientific World Journal},
  year = {2025},
  doi = {10.1155/tswj/3581428}
}
Kostenlos starten →