Corrosion Rate of Medium‐Carbon Steel Quenched in Nanofluids (Al 2 O 3 and CuO) at Different Temperatures

Nervana Abbas Abd, M. Hanafy, Amr Abdelghany, Hani Aziz Amen

International Journal of Corrosion · 2024-01 · 2024 (1)

DOI: 10.1155/ijco/5531986 ↗

Kurz gefasst

Fachartikel in der Zeitschrift International Journal of Corrosion, online erschienen am 12.12.2024. Verfasst von Nervana Abbas Abd und 3 weiteren Autor:innen. Die Arbeit wurde bisher 3-mal zitiert (Crossref) und nennt 33 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The corrosion of carbon steel pipelines and storage tanks is a common occurrence in the oil and gas industry. To reduce metal corrosion, we examined the effect of quenching medium‐carbon steel in nanofluids. Medium‐carbon steel was quenched, firstly; heated to above the normal recrystallisation temperature for a sufficient time to allow the heat to penetrate the metal; and then cooled down quickly in tap water or alumina (Al 2 O 3 ) or copper oxide (CuO) nanofluid with a volume concentration of 0.05%. Some specimens were then tempered. To investigate the different phases before corrosion tests such as ferrite–cementite and ferrite–martensite with a small amount of retained austenite, X‐ray diffraction images are used. Furthermore, the dislocation density and grain size of the quenched steel were obtained, which played an important role in determining the corrosion behaviour. Finally, all specimens were quenched and immersed in 3.5% sodium chloride (NaCl) aqueous solution saturated or NaCl saturated with carbon dioxide (CO 2 ) at a temperature of 25°C, 35°C, 45°C, or 55°C. The morphology of the steel surface was observed by scanning electron microscopy after the corrosion tests. The number of pits on the surface was found to vary with the heat treatment and corrosion conditions. The results showed that both the cathodic Tafel slope β c and the anodic Tafel slope β a decrease with increasing temperature due to the formation of a layer of iron oxide (Fe 2 O 3 ), which prevented chlorine ions (Cl − ) from reaching the surface of the metal and causing corrosion. Thus, the corrosion current density ( I corr ) decreased with increasing temperature. It was found that the corrosion efficiency is highest when quenched with CuO solution and then tempered (CuO + T) where it was 86.677% at 55°C. Above this temperature, there was little change in the effectiveness. Low‐temperature tests damage the metal; moreover, the corrosion products that formed were loose and porous when the quenched metal was exposed to CO 2 because the temperature was too low for a protective film to be formed. Experimental observations indicate that the corrosion resistance of medium‐carbon steel quenched in CuO nanofluid is greater than that of the steel quenched in Al 2 O 3 nanofluid under the same conditions. In addition, the corrosion characteristics differed between the quenching and tempered steel and the steel that was only quenched.

Zitieren

APA

Abd, N. A., Hanafy, M., Abdelghany, A., & Amen, H. A. (2024). Corrosion Rate of Medium‐Carbon Steel Quenched in Nanofluids (Al 2 O 3 and CuO) at Different Temperatures. International Journal of Corrosion, 2024(1). https://doi.org/10.1155/ijco/5531986

Vancouver

Abd NA, Hanafy M, Abdelghany A, Amen HA. Corrosion Rate of Medium‐Carbon Steel Quenched in Nanofluids (Al 2 O 3 and CuO) at Different Temperatures. International Journal of Corrosion. 2024;2024(1). doi:10.1155/ijco/5531986

BibTeX
@article{Abd2024,
  author = {Abd, Nervana Abbas and Hanafy, M. and Abdelghany, Amr and Amen, Hani Aziz},
  title = {Corrosion Rate of Medium‐Carbon Steel Quenched in Nanofluids (Al 2 O 3 and CuO) at Different Temperatures},
  journal = {International Journal of Corrosion},
  year = {2024},
  volume = {2024},
  number = {1},
  doi = {10.1155/ijco/5531986}
}
Kostenlos starten →