High-Temperature Wear Performance of Laser-Cladded NiCrBSi/60 wt% WC Composite Coating on SS316L Alloy
Journal of Tribology · 01.12.2025 · 147 (12)
DOI: 10.1115/1.4069258 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Tribology, online erschienen am 25.08.2025. Verfasst von Lakshmi Manasa Birada und 3 weiteren Autor:innen. Die Arbeit wurde bisher 4-mal zitiert (Crossref) und nennt 37 Literaturangaben.
Abstract (Originalsprache)
This investigation reports on the processing and characterization of NiCrBSi/60 wt% WC composite claddings on SS316L steel substrates by laser cladding process. Microstructural analyses conducted using a scanning electron microscope, an energy dispersive spectrometer, and X-ray diffraction confirmed the successful development of dense cladding layers containing WC reinforcement phases. Microhardness testing revealed a substantial increase in hardness within the clad layer, reaching approximately 1086 HV0.2, significantly higher than the 190 HV0.2 of the SS316L. As the testing temperature increases, the wear-rate and the coefficient of friction (COF) of the coated sample decrease, making it applicable in high-temperature applications. The observed reduction in the COF at higher testing temperatures is attributed to the formation of a lubricious oxide layer that serves as a protective barrier, preventing direct contact between the coated sample and the hard counter disc. Tribological experiments conducted at room temperature, 350 °C, and 700 °C demonstrated a progressive increase in wear-rate with temperature, especially beyond 350 °C, attributed to thermal softening, oxide layer formation, and wear transformations. At 700 °C, oxidation and delamination were the prominent mechanisms. Compared to room temperature, wear resistance decreased by 559.5% at 700 °C, with reductions of 381.1% observed at 350 °C. These findings underscore the critical role of WC reinforcements in retaining wear resistance up to 350 °C. Conversely, at 700 °C, intensified oxidation and matrix softening led to an enhanced coefficient of friction till stabilization occurred after approximately 150 m of sliding distance.
Zitieren
APA
Birada, L. M., Karthik, M. R., Babu, M. S., & Kumar, G. P. (2025). High-Temperature Wear Performance of Laser-Cladded NiCrBSi/60 wt% WC Composite Coating on SS316L Alloy. Journal of Tribology, 147(12). https://doi.org/10.1115/1.4069258
Vancouver
Birada LM, Karthik MR, Babu MS, Kumar GP. High-Temperature Wear Performance of Laser-Cladded NiCrBSi/60 wt% WC Composite Coating on SS316L Alloy. Journal of Tribology. 2025;147(12). doi:10.1115/1.4069258
BibTeX
@article{Birada2025,
author = {Birada, Lakshmi Manasa and Karthik, Mondi Rama and Babu, Mulpur Sarat and Kumar, G. Pavan},
title = {High-Temperature Wear Performance of Laser-Cladded NiCrBSi/60 wt% WC Composite Coating on SS316L Alloy},
journal = {Journal of Tribology},
year = {2025},
volume = {147},
number = {12},
doi = {10.1115/1.4069258}
}
EUVIMED