Curing Capacity of Band‐Bonding Resinous Adhesives Under 3D ‐Printed Molar Bands

Sofia Sideri, Maria Dimitriadi iD, Nearchos Panayi iD, Spyridon N Papageorgiou iD, Theodore Eliades iD, George Eliades iD

Orthodontics & Craniofacial Research · 2026-10-25

DOI: 10.1111/ocr.70190 ↗

At a glance

Journal article in Orthodontics & Craniofacial Research, published online on 2026-10-25. Written by Sofia Sideri and 5 co-authors. Institution: Department of Biomaterials, School of Dentistry, National and Kapodistrian University of Athens, Athens, Greece. 33 references. The full text is freely available (open access, CC BY 4.0).

AbstractSubjectsBibliografiske oplysningerCiteRelated studies

Abstract (original language)

Aim

To evaluate the curing efficiency of three resin composite adhesives applied beneath 3D‐printed molar bands, by determining their degree of conversion (DC%) at different depths. Materials and Methods Fifteen 3D‐printed metallic band specimens were divided into three groups and bonded with Band Lock Blue (BLB), Optiband Ultra Blue (OBU), or Transbond Plus (TRP). Adhesives were applied in 150 μm films and light‐cured for 30 s (1200 mW/cm 2 ). Degree of conversion (DC%) was measured at the top, middle, and bottom regions using attenuated total reflection Fourier‐transform infrared spectroscopy (ATR‐FTIR). Directly irradiated specimens served as controls. Statistical analysis of DC% values was performed with regression modelling at a 5% level.

Results

A reduction in conversion beneath the bands compared to non‐banded controls was seen, which was dependent on both the adhesive type and the region. For BLB, equally low DC% values were found for banded and non‐banded specimens across all regions. Banded OBU specimens had significantly lower DC% compared to non‐banded controls at all regions. Finally, TRP banded specimens had significantly lower DC% compared to non‐banded controls at the middle and bottom regions, but not at the top region.

Conclusions

Curing capacity of band adhesives under 3D‐printed bands is material‐dependent. Blue‐shaded OBU and dual‐cured BLB showed more uniform conversion, whereas white‐shaded TRP exhibited significant depth variations. However, conversion of the adhesives tested under 3D‐printed metallic bands was acceptable when a high‐intensity light‐curing unit was used for an extended irradiation time for orthodontic applications (30 s).

Subjects

Author keywords

3D‐printed molar bandsdegree of conversionlight‐curing efficiencyorthodontic adhesivesresin composite curing

Authors and institutions

  • Department of Biomaterials, School of Dentistry, National and Kapodistrian University of Athens, Athens, Greece.
  • Faculty of Dentistry, Department of Orthodontics, European University Cyprus, Nicosia, Cyprus.
  • Clinic of Orthodontics and Pediatric Dentistry, University of Zurich, Center for Dental Medicine, Zurich, Switzerland.

ORCID profiles: Maria Dimitriadi, Nearchos Panayi, Spyridon N Papageorgiou, Theodore Eliades, George Eliades

Cite

APA

Sideri, S., Dimitriadi, M., Panayi, N., Papageorgiou, S. N., Eliades, T., & Eliades, G. (2026). Curing Capacity of Band‐Bonding Resinous Adhesives Under 3D ‐Printed Molar Bands. Orthodontics & Craniofacial Research. https://doi.org/10.1111/ocr.70190

Vancouver

Sideri S, Dimitriadi M, Panayi N, Papageorgiou SN, Eliades T, Eliades G. Curing Capacity of Band‐Bonding Resinous Adhesives Under 3D ‐Printed Molar Bands. Orthodontics & Craniofacial Research. 2026. doi:10.1111/ocr.70190

BibTeX
@article{Sideri2026,
  author = {Sideri, Sofia and Dimitriadi, Maria and Panayi, Nearchos and Papageorgiou, Spyridon N and Eliades, Theodore and Eliades, George},
  title = {Curing Capacity of Band‐Bonding Resinous Adhesives Under 3D ‐Printed Molar Bands},
  journal = {Orthodontics & Craniofacial Research},
  year = {2026},
  doi = {10.1111/ocr.70190}
}
Start for free →