Qualitative SEM analysis of fracture surfaces for dental ceramics and polymers broken by flexural strength testing and crown compression

Tariq F Alghazzawi iD, Gregg M Janowski, Haibin Ning, Alan W Eberhardt

Journal of Prosthodontics · 2023

DOI: 10.1111/jopr.13659 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Prosthodontics, 2023. Verfasst von Tariq F Alghazzawi und 3 weiteren Autor:innen. Beteiligte Einrichtung: Department of Substitutive Dental Sciences, Taibah University, Madina, Saudi Arabia. Hauptthemen laut MEDLINE: Dental Porcelain, Flexural Strength. Die Arbeit wurde bisher 33-mal zitiert (Crossref) und nennt 37 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0). Gefördert von: Fulbright Visiting Scholar Program, The Bureau of Educational and Cultural Affairs, United States Department of State with cooperation of the Institute of International Education.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Purpose

To perform qualitative analysis using scanning electron microscopy (SEM) of fracture surfaces for ceramic and polymeric dental materials broken via standardized flexural and crunch‐the‐crown (CTC) tests. Materials and Methods Zirconia, glass–ceramic, and polymeric (Trilor; TRI, Juvora; JUV, Pekkton; PEK) materials were loaded using crowns for CTC tests, discs (zirconia and glass–ceramics) for piston‐on‐3 ball tests, bars (polymer) for 3‐point bend tests, and bars (zirconia, glass–ceramics) for 4‐point bend tests. SEM was used to characterize the fracture surfaces and identify fracture surface features (e.g., origin, mist, hackle, and the direction of crack propagation [DCP]). Electron dispersive spectroscopy was used to identify the local chemistry.

Results

Fracture surface features were found to be less visually apparent for glass–ceramics than zirconia. For zirconia bars, fractures originated roughly midway between the corner and center for processing defects related to sintering. Fractures originated at the bottom corners of glass–ceramic bars (void or surface flaw) and PEK bars (surface flaw). TRI bar failures exposed glassy fibers. Fracture features were generally less discernable for discs compared to bars for zirconia and glass–ceramics. Ceramic crowns fractured into 2 to 3 pieces, with fractures originating at the occlusal surface and clear evidence for the DCP. Failures of TRI and JUV specimens (bars and crowns) were less catastrophic than for the ceramics, with exposed fibers (TRI) and surface cracks (JUV). PEK crown and bar fractures presented dimple (ductile) features formed due to microvoid coalescence followed by brittle crack propagation.

Conclusions

The critical flaws responsible for failure initiation were a function of material composition and test configuration. Fractographic analysis can reveal problems associated with the manufacturing of materials, their handling, grinding and finishing/polishing procedures, the structural design and choice of material, and the quality of the final laboratory‐delivered restoration.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

Dental PorcelainFlexural StrengthMicroscopy, Electron, ScanningMaterials TestingCeramicsCrownsZirconiumSurface PropertiesDental Restoration FailureDental Stress Analysis

Stichwörter der Autor:innen

SEMcrackfailure originflawfractographyfracture

Substanzen

Dental Porcelainzirconium oxideZirconium

Autor:innen und Institutionen

  • Department of Substitutive Dental Sciences, Taibah University, Madina, Saudi Arabia.
  • Department of Mechanical and Materials Engineering, The University of Alabama at Birmingham, Birmingham, Alabama, USA.
  • Department of Biomedical Engineering, The University of Alabama at Birmingham, Birmingham, Alabama, USA.

ORCID-Profile: Tariq F Alghazzawi

Förderung

  • Fulbright Visiting Scholar Program
  • The Bureau of Educational and Cultural Affairs
  • United States Department of State with cooperation of the Institute of International Education

Zitieren

APA

Alghazzawi, T. F., Janowski, G. M., Ning, H., & Eberhardt, A. W. (2023). Qualitative SEM analysis of fracture surfaces for dental ceramics and polymers broken by flexural strength testing and crown compression. Journal of Prosthodontics. https://doi.org/10.1111/jopr.13659

Vancouver

Alghazzawi TF, Janowski GM, Ning H, Eberhardt AW. Qualitative SEM analysis of fracture surfaces for dental ceramics and polymers broken by flexural strength testing and crown compression. Journal of Prosthodontics. 2023. doi:10.1111/jopr.13659

BibTeX
@article{Alghazzawi2023,
  author = {Alghazzawi, Tariq F and Janowski, Gregg M and Ning, Haibin and Eberhardt, Alan W},
  title = {Qualitative SEM analysis of fracture surfaces for dental ceramics and polymers broken by flexural strength testing and crown compression},
  journal = {Journal of Prosthodontics},
  year = {2023},
  doi = {10.1111/jopr.13659}
}
Kostenlos starten →