Edge Chipping Resistance and Flexural Strength of CAD ‐ CAM Ceramics Before and After Thermomechanical Aging
Journal of Esthetic and Restorative Dentistry · 2025
DOI: 10.1111/jerd.13391 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Esthetic and Restorative Dentistry, 2025. Verfasst von Min-Gyu Song und 4 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthodontics and Research Institute of Oral Science, College of Dentistry, Gangneung-Wonju National University, Gangneung, Republic o…. Hauptthemen laut MEDLINE: Flexural Strength, Computer-Aided Design, Ceramics, Dental Porcelain. Die Arbeit wurde bisher 7-mal zitiert (Crossref) und nennt 43 Literaturangaben. Gefördert von: National Research Foundation of Korea.
Abstract (Originalsprache)
Objectives
To evaluate the complementary mechanical properties of dental ceramics using edge chipping resistance (Rea) and flexural strength before and after thermomechanical aging. Material and Methods Computer‐aided design and computer‐aided manufacturing of ceramic materials, including zirconia (ZR), lithium disilicate (LS2), and resin nanoceramics (RNC), were evaluated. Specimens for flexural strength testing were fabricated with dimensions of 3 × 4 × 25 mm, with 30 specimens per group. For the edge chipping test (ECT), specimens were fabricated with dimensions of 3 × 4 × 12 mm, with 48 specimens per group. Half of the specimens for both tests were subjected to thermomechanical aging for 200,000 cycles at 50 N. A Weibull analysis was performed to determine flexural strength. Fractographic analysis was performed before and after thermomechanical aging during the ECT. X‐ray diffractometry (XRD) was performed on the ZR specimens before and after thermomechanical aging. Flexural strength was analyzed using a two‐way repeated analysis of variance (ANOVA) with a t ‐test, and Rea was analyzed using Pearson correlation and a two‐way repeated ANOVA.
Results
The flexural strength and Rea differed according to the material ( p = 0.001), whereas they were similar before and after thermomechanical aging ( p > 0.05). The Weibull modulus of the flexural strength decreased after thermomechanical aging. In the fractographic analysis of the ECT, more than two fracture origins were identified after thermomechanical aging. The XRD analysis of ZR showed an increased monoclinic phase after thermomechanical aging.
Conclusion
All the materials met the ISO 6872 standards for bending test. However, LS2 and RNC show low edge chipping resistance within the range of the occlusal force. The thermomechanical aging did not significantly alter the mechanical properties of the materials. However, the Weibull coefficients of the flexural strength decreased, and an additional origin of fracture appeared after thermomechanical aging. Significance Flexural strength and Rea differed depending on the material used. The probability of the material fracture increased after thermomechanical aging. To understand ceramic fractures, two mechanical tests and thermomechanical aging must be performed together.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Department of Prosthodontics and Research Institute of Oral Science, College of Dentistry, Gangneung-Wonju National University, Gangneung, Republic of Korea.
ORCID-Profile: Min-Gyu Song, Kyung-Ho Ko, Yoon-Hyuk Huh, Chan-Jin Park, Lee-Ra Cho
Förderung
- National Research Foundation of Korea
Zitieren
APA
Song, M. G., Ko, K. H., Huh, Y. H., Park, C. J., & Cho, L. R. (2025). Edge Chipping Resistance and Flexural Strength of CAD ‐ CAM Ceramics Before and After Thermomechanical Aging. Journal of Esthetic and Restorative Dentistry. https://doi.org/10.1111/jerd.13391
Vancouver
Song MG, Ko KH, Huh YH, Park CJ, Cho LR. Edge Chipping Resistance and Flexural Strength of CAD ‐ CAM Ceramics Before and After Thermomechanical Aging. Journal of Esthetic and Restorative Dentistry. 2025. doi:10.1111/jerd.13391
BibTeX
@article{Song2025,
author = {Song, Min-Gyu and Ko, Kyung-Ho and Huh, Yoon-Hyuk and Park, Chan-Jin and Cho, Lee-Ra},
title = {Edge Chipping Resistance and Flexural Strength of CAD ‐ CAM Ceramics Before and After Thermomechanical Aging},
journal = {Journal of Esthetic and Restorative Dentistry},
year = {2025},
doi = {10.1111/jerd.13391}
}
EUVIMED