Epoxy Evaluation for Mechanical Integration of Cryogenic Detector in the Focal Plane of X-IFU Instrument of ATHENA
IEEE Transactions on Applied Superconductivity · 2026-09 · 36 (6) · 1-5
DOI: 10.1109/tasc.2026.3678093 ↗Kurz gefasst
Fachartikel in der Zeitschrift IEEE Transactions on Applied Superconductivity, 2026-09. Verfasst von Kifayat Ullah Khan Niazi und 11 weiteren Autor:innen. Gefördert von: Italian Space Agency.
Abstract (Originalsprache)
Space-borne equipment undergoes extreme environmental conditions affecting the structural integrity and overall working of the systems, particularly the parts joined using adhesives. In this article, we present the investigation done for CryoAC glue evaluation for structural models under development for the focal plane assembly (FPA) of future space missions such as ATHENA, which will operate at 50 mK temperature in space. Since these silicon detectors are mounted on copper brackets using adhesive bonds, understanding glue behavior under extreme operational conditions is critical. Three adhesive candidates, namely, STYCAST 2850FT/24LV, EC-9323 B/A (pink glue), EC-2216 B/A (grey glue) have been tested to be qualified for future use in space missions against a predefined qualification criterion. Silicon chips (11 × 11 mm, 1.5 mm thick) were bonded to rough copper surfaces and subjected to standard lap shear testing. Samples were prepared using two curing methods: Room temperature long curing and fast curing in hot oven (except STYCAST 2850FT). The campaign is divided into two parts, the first batch includes curing of glue, three samples each, and subjected to lap shear testing whereas second part includes low temperature thermal cycling (4–300 K) before lap shear testing. Among the three candidates, only EC-2216 oven cured satisfied all qualification criteria, with
Förderung
- Italian Space Agency
Zitieren
APA
Niazi, K. U. K., Rigano, M., Bianco, F., Barusso, L. F., Grosso, D., Benvenuto, L., Benvenuto, M., Lertora, E., Celasco, E., Villa, F., Lapolla, M., & Gatti, F. (2026). Epoxy Evaluation for Mechanical Integration of Cryogenic Detector in the Focal Plane of X-IFU Instrument of ATHENA. IEEE Transactions on Applied Superconductivity, 36(6), 1-5. https://doi.org/10.1109/tasc.2026.3678093
Vancouver
Niazi KUK, Rigano M, Bianco F, Barusso LF, Grosso D, Benvenuto L, et al. Epoxy Evaluation for Mechanical Integration of Cryogenic Detector in the Focal Plane of X-IFU Instrument of ATHENA. IEEE Transactions on Applied Superconductivity. 2026;36(6):1-5. doi:10.1109/tasc.2026.3678093
BibTeX
@article{Niazi2026,
author = {Niazi, Kifayat Ullah Khan and Rigano, Manuela and Bianco, Federico and Barusso, Lorenzo Ferrari and Grosso, Daniele and Benvenuto, Luigi and Benvenuto, Matteo and Lertora, Enrico and Celasco, Edvige and Villa, Francesco and Lapolla, Marco and Gatti, Flavio},
title = {Epoxy Evaluation for Mechanical Integration of Cryogenic Detector in the Focal Plane of X-IFU Instrument of ATHENA},
journal = {IEEE Transactions on Applied Superconductivity},
year = {2026},
volume = {36},
number = {6},
pages = {1--5},
doi = {10.1109/tasc.2026.3678093}
}
EUVIMED