Abstract (Originalsprache)
Metals have long dominated orthopedic implants due to their high strength, but their elastic modulus greatly exceeds that of bone, causing stress shielding, bone resorption, and implant loosening. Polymers better match bone elasticity but lack sufficient long-term mechanical strength. Carbon fiber-reinforced PEEK (CFR-PEEK) provides an optimal balance, combining bone-like elasticity with high tensile strength. Its compatibility with fused filament fabrication (FFF) enables the fabrication of low-cost, patient-specific implants. CFR-PEEK tensile specimens were made using the technique of FFF by varying three critical process parameters: (i) infill geometry [hexagonal, grid, and triangular], (ii) infill density [50%, 70%, and 90%], and (iii) layer thickness [0.1 mm, 0.2 mm, and 0.3 mm]. The test specimens were deformed under the influence of uniaxial tensile loading very much in conformance with procedures detailed in the ASTM D3039 standard for the purpose of evaluating mechanical performance. A life cycle assessment (LCA) was conducted to estimate embodied energy and carbon dioxide (CO 2 ) emission associated with each fabrication condition. Hexagonal infill geometry exhibited superior load distribution and bonding efficiency when compared to the grid pattern and the triangular pattern. Higher infill density did improve both the tensile strength and stiffness due to reduced porosity. An optimum combination of hexagonal geometry, 90% infill density, and 0.1 mm layer thickness did provide maximum tensile strength and structural integrity. Life cycle assessment (LCA) results indicated that a higher infill density led to an increase in embodied energy and CO 2 emissions.
Zitieren
APA
Aryan, O. R., Dubey, A. D., Debnath, K., Dutta, H., & Srivatsan, T. S. (2026). Mechanical evaluation and life cycle assessment of fused filament fabricated carbon fiber-reinforced polyether ether ketone [CFR-PEEK] composite for orthopedic implant application. Physica Scripta, 101(15), 155908. https://doi.org/10.1088/1402-4896/ae5af0
Vancouver
Aryan OR, Dubey AD, Debnath K, Dutta H, Srivatsan TS. Mechanical evaluation and life cycle assessment of fused filament fabricated carbon fiber-reinforced polyether ether ketone [CFR-PEEK] composite for orthopedic implant application. Physica Scripta. 2026;101(15):155908. doi:10.1088/1402-4896/ae5af0
BibTeX
@article{Aryan2026,
author = {Aryan, Omkar Raj and Dubey, Ankit Dhar and Debnath, Kishore and Dutta, Hrishikesh and Srivatsan, T S},
title = {Mechanical evaluation and life cycle assessment of fused filament fabricated carbon fiber-reinforced polyether ether ketone [CFR-PEEK] composite for orthopedic implant application},