EUVIMEDEUVIMED entdecken
Crossref

Modeling galvanic corrosion of 316L/40Cr and Ni–P coated 42CrMo alloys in downhole produced water corrosion environment

Dawei Ai, Zhonglong Shi, Zheng Sun, Tianle Li, Daiyan Zhang, Ziqiang Wang, Zhikun Wang, Yu Fu, Xiao Tang, Songqing Hu

Modelling and Simulation in Materials Science and Engineering · 15.06.2025 · 33 (4) · 045003

DOI: 10.1088/1361-651x/adc9cd ↗

Kurz gefasst

Fachartikel in der Zeitschrift Modelling and Simulation in Materials Science and Engineering, online erschienen am 16.04.2025. Verfasst von Dawei Ai und 9 weiteren Autor:innen. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 36 Literaturangaben. Gefördert von: National Natural Science Foundation of China, Shandong Province Youth Entrepreneurship Technology Support Program for Higher Education Institutions, Applied Research Project of Qingdao Postdoctoral Researchers.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Water originating from underground frequently leads to severe corrosion of subsurface equipment and tubing, increasing the risks of structural failure, pipeline leakage, and environmental contamination, which can endanger both operational safety and environmental integrity. To delve into the galvanic corrosion of downhole equipment and tubing, a comprehensive study was conducted using COMSOL simulations to explore the galvanic corrosion mechanism between 316L/40Cr and Ni–P coated 42CrMo alloys. According to the electrochemical tests, a two-dimensional galvanic corrosion model encompassing 316L/40Cr, Ni–P coating, and 42CrMo substrate was established. The mechanisms of galvanic corrosion under varying material and coating damage scenarios were extensively discussed and analyzed. The findings reveal that, when the Ni–P coating remains intact, 40Cr undergoes more pronounced corrosion (approximately 35.3 µ m) compared to 316L (about 2.11 µ m). However, upon coating damage, 316L becomes the cathode, while 40Cr and 42CrMo function as anodes. Notably, the total current in the coupled system (0.475 mA) comprising 316L, 42CrMo, and Ni–P coating is lower than that in the system (0.712 mA) with 40Cr, 42CrMo, and Ni–P coating. Additionally, an increase in the surface area of the 316L electrode correlates with an enhanced corrosion rate, manifesting in corrosion depths of 32.09–32.16 µ m, 31.3–31.2 µ m, and 30.172–30.312 µ m at 400, 300, and 200 µ m, respectively.

Förderung

  • National Natural Science Foundation of China
  • Shandong Province Youth Entrepreneurship Technology Support Program for Higher Education Institutions
  • Applied Research Project of Qingdao Postdoctoral Researchers
  • Fundamental Research Funds for the Central Universities

Zitieren

APA

Ai, D., Shi, Z., Sun, Z., Li, T., Zhang, D., Wang, Z., Wang, Z., Fu, Y., Tang, X., & Hu, S. (2025). Modeling galvanic corrosion of 316L/40Cr and Ni–P coated 42CrMo alloys in downhole produced water corrosion environment. Modelling and Simulation in Materials Science and Engineering, 33(4), 045003. https://doi.org/10.1088/1361-651x/adc9cd

Vancouver

Ai D, Shi Z, Sun Z, Li T, Zhang D, Wang Z, et al. Modeling galvanic corrosion of 316L/40Cr and Ni–P coated 42CrMo alloys in downhole produced water corrosion environment. Modelling and Simulation in Materials Science and Engineering. 2025;33(4):045003. doi:10.1088/1361-651x/adc9cd

BibTeX
@article{Ai2025,
  author = {Ai, Dawei and Shi, Zhonglong and Sun, Zheng and Li, Tianle and Zhang, Daiyan and Wang, Ziqiang and Wang, Zhikun and Fu, Yu and Tang, Xiao and Hu, Songqing},
  title = {Modeling galvanic corrosion of 316L/40Cr and Ni–P coated 42CrMo alloys in downhole produced water corrosion environment},
  journal = {Modelling and Simulation in Materials Science and Engineering},
  year = {2025},
  volume = {33},
  number = {4},
  pages = {045003},
  doi = {10.1088/1361-651x/adc9cd}
}
Kostenlos starten →