Metal–organic chemical vapor deposition of p-type NiO and NiO/β-Ga2O3 PN diodes
APL Electronic Devices · 01.12.2025 · 1 (4)
DOI: 10.1063/5.0285513 ↗Kurz gefasst
Fachartikel in der Zeitschrift APL Electronic Devices, online erschienen am 01.10.2025. Verfasst von Dong Su Yu und 5 weiteren Autor:innen. Die Arbeit wurde bisher 4-mal zitiert (Crossref) und nennt 75 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC 4.0). Gefördert von: Air Force Office of Scientific Research, National Science Foundation, Advanced Research Projects Agency-Energy.
Abstract (Originalsprache)
In this work, p-type NiO thin films were grown on (010) β-Ga2O3 substrates via metal–organic chemical vapor deposition (MOCVD). The growth conditions, including Ni(dmamb)2 (Ni precursor) molar flow rate, oxygen flow rate, and growth temperature, were systematically tuned to achieve p-type NiO thin films. With a relatively high O2 flow rate of 10 000 sccm, the grown NiO film exhibited smooth surface morphologies with a root mean square roughness value of 2.39 nm. The measured hole concentration ranged from 1 × 1016 to 4.5 × 1016 cm−3, with room-temperature mobility varying between 3 and 1.7 cm2/V s. Cross-sectional scanning transmission electron microscopy imaging and analysis revealed a NiGa2O4 interfacial layer formed between the p-type NiO thin film and β-Ga2O3 substrate, due to Ni diffusion. Given the challenges of achieving p-type conductivity in β-Ga2O3, NiO has emerged as a potential alternative material. Furthermore, in situ MOCVD grown NiO/β-Ga2O3 heterojunction was used to fabricate PN diodes with two different diameters: 100 and 200 μm. This study represents the first demonstration of all-MOCVD growth of p-NiO/β-Ga2O3 PN diodes on (010) Sn-doped β-Ga2O3 substrates. Compared to radio frequency sputtering and atomic layer deposition of p-NiO, MOCVD allows the continuous growth of p-NiO on top of Ga2O3, which can potentially suppress interface defects and impurity contamination. The breakdown voltages of the MOCVD grown NiO/β-Ga2O3 PN diodes were measured as 348 and 267 V for the 100 and 200 μm diameter devices, respectively. The knee voltages (Vknee) were extracted as 4.7–5.2 V.
Förderung
- Air Force Office of Scientific Research
- National Science Foundation
- Advanced Research Projects Agency-Energy
Zitieren
APA
Yu, D. S., Meng, L., Vangipuram, V. G. T., Chae, C., Hwang, J., & Zhao, H. (2025). Metal–organic chemical vapor deposition of p-type NiO and NiO/β-Ga2O3 PN diodes. APL Electronic Devices, 1(4). https://doi.org/10.1063/5.0285513
Vancouver
Yu DS, Meng L, Vangipuram VGT, Chae C, Hwang J, Zhao H. Metal–organic chemical vapor deposition of p-type NiO and NiO/β-Ga2O3 PN diodes. APL Electronic Devices. 2025;1(4). doi:10.1063/5.0285513
BibTeX
@article{Yu2025,
author = {Yu, Dong Su and Meng, Lingyu and Vangipuram, Vijay Gopal Thirupakuzi and Chae, Christopher and Hwang, Jinwoo and Zhao, Hongping},
title = {Metal–organic chemical vapor deposition of p-type NiO and NiO/β-Ga2O3 PN diodes},
journal = {APL Electronic Devices},
year = {2025},
volume = {1},
number = {4},
doi = {10.1063/5.0285513}
}