Wendi Zhang, Dunbo Yu, Weibin Cui, Xiaojun Sun, Yuanfei Yang, Xiao Lin, Qingjia Wang, Yang Luo, Zilong Wang

Applied Physics Letters · 2025-03-01 · 126 (12)

DOI: 10.1063/5.0247741 ↗

At a glance

Journal article in Applied Physics Letters, published online on 2025-03-25. Written by Wendi Zhang and 8 co-authors. Cited 7 times so far (Crossref); 22 references. Funded by: National Key Research and Development Program of China, National Natural Science Foundation of China, Key Research and Development Program of Shandong Province.

AbstraktBibliografické údajeCiteRelated studies

Abstract (original language)

During the grain boundary diffusion (GBD) of Tb, the core–shell and reverse core–shell structures are the two main microstructures influencing the magnetic properties of the sintered Nd-Fe-B magnets. These two microstructures are all composed of the (Nd, Tb)2Fe14B phase, but the formation mechanisms are different. The difference in formation mechanism of the core–shell and reverse core–shell structures was studied by quenching the magnets at different temperatures and holding times. The (Nd, Tb)2Fe14B shell of the core–shell structure is the precondition for forming the reverse core–shell structure. The triple-junction phases (TJPs) area change proves that the Nd elements diffuse from the TJPs to the surface of the (Nd, Tb)2Fe14B shell to form the Tb-poor shell in the reverse core–shell structure and the Gaussian distribution of Tb in the shell of the core–shell structure. In addition, the difference in the Tb content distribution leads to different demagnetization processes, resulting in the opposite effect of these two microstructures on the coercivity. The GBD aims to increase the entire coercivity by enhancing the surface anisotropy field (HA), such as the Tb-rich shell for the grains and the Tb-rich surface (∼200 μm) for the magnets. Therefore, for the reverse core–shell structure forming in the surface of the magnets, the surface with a low HA decreases the coercivity of the grains, reducing the coercivity of the magnets.

Funding

  • National Key Research and Development Program of China
  • National Natural Science Foundation of China
  • Key Research and Development Program of Shandong Province
  • National Youth Talent Support Program

Cite

APA

Zhang, W., Yu, D., Cui, W., Sun, X., Yang, Y., Lin, X., Wang, Q., Luo, Y., & Wang, Z. (2025). Study on the difference in formation mechanism and demagnetization process between core–shell and reverse core–shell structures of sintered Nd-Fe-B magnets diffused with Tb. Applied Physics Letters, 126(12). https://doi.org/10.1063/5.0247741

Vancouver

Zhang W, Yu D, Cui W, Sun X, Yang Y, Lin X, et al. Study on the difference in formation mechanism and demagnetization process between core–shell and reverse core–shell structures of sintered Nd-Fe-B magnets diffused with Tb. Applied Physics Letters. 2025;126(12). doi:10.1063/5.0247741

BibTeX
@article{Zhang2025,
  author = {Zhang, Wendi and Yu, Dunbo and Cui, Weibin and Sun, Xiaojun and Yang, Yuanfei and Lin, Xiao and Wang, Qingjia and Luo, Yang and Wang, Zilong},
  title = {Study on the difference in formation mechanism and demagnetization process between core–shell and reverse core–shell structures of sintered Nd-Fe-B magnets diffused with Tb},
  journal = {Applied Physics Letters},
  year = {2025},
  volume = {126},
  number = {12},
  doi = {10.1063/5.0247741}
}
Start for free →