Kurz gefasst

Fachartikel in der Zeitschrift Scientific Reports, online erschienen am 11.05.2024. Verfasst von Yuanmin Zou und 4 weiteren Autor:innen. Beteiligte Einrichtung: Department of Chemical and Metallurgical Engineering, School of Chemical Engineering, Aalto University, 00076, Aalto, Finland. Die Arbeit wurde bisher 35-mal zitiert (Crossref) und nennt 51 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: BATCircle2.0 project.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study focuses on the effect of an emerging source of waste, lithium iron phosphate (LFP) cathode materials, on the hydrometallurgical recycling of the currently dominant industrial battery waste that is rich in transition metals (Ni, Co, Mn, and Li). The effects of the dosage of LFP, initial acidity, and timing of LFP reductant addition were investigated in sulfuric acid (H 2 SO 4 ) leaching ( t = 3 h, T = 60 °C, ω = 300 rpm). The results showed that addition of LFP increased both transition metal extraction and acid consumption. Further, the redox potential was lowered due to the increased presence of Fe 2+ . An initial acidity of 2.0 mol/L H 2 SO 4 with acid consumption of 1.3 kg H 2 SO 4 /kg black mass provided optimal conditions for achieving a high leaching yield (Co = 100%, Ni = 87.6%, Mn = 91.1%, Li = 100%) and creating process solutions (Co 8.8 g/L, Ni 13.8 g/L, Li 6.7 g/L, Mn 7.6 g/L, P 12.1 g/L) favorable for subsequent hydrometallurgical processing. Additionally, the overall efficiency of H 2 O 2 decreased due to its decomposition by high concentrations of Fe 2+ and Mn 2+ when H 2 O 2 was added after t = 2 h, leading to only a minor increase in final battery metals extraction levels.

Schlagwörter

Stichwörter der Autor:innen

Battery recyclingCathode active materialLeachingLithium-ion batteryReductant

Autor:innen und Institutionen

  • Department of Chemical and Metallurgical Engineering, School of Chemical Engineering, Aalto University, 00076, Aalto, Finland.
  • Metso Outotec Research Center, Kuparitie 10, 28101, Pori, Finland.
  • Department of Chemical and Metallurgical Engineering, School of Chemical Engineering, Aalto University, 00076, Aalto, Finland. mari.lundstrom@aalto.fi.

Förderung

  • BATCircle2.0 project

Zitieren

APA

Zou, Y., Chernyaev, A., Ossama, M., Seisko, S., & Lundström, M. (2024). Leaching of NMC industrial black mass in the presence of LFP. Scientific Reports, 14(1). https://doi.org/10.1038/s41598-024-61569-3

Vancouver

Zou Y, Chernyaev A, Ossama M, Seisko S, Lundström M. Leaching of NMC industrial black mass in the presence of LFP. Scientific Reports. 2024;14(1). doi:10.1038/s41598-024-61569-3

BibTeX
@article{Zou2024,
  author = {Zou, Yuanmin and Chernyaev, Alexander and Ossama, Muhammad and Seisko, Sipi and Lundström, Mari},
  title = {Leaching of NMC industrial black mass in the presence of LFP},
  journal = {Scientific Reports},
  year = {2024},
  volume = {14},
  number = {1},
  doi = {10.1038/s41598-024-61569-3}
}
Kostenlos starten →