Biomimetic Mg-Regulated Mineralization of Aragonite Laths for High-Strength and Fire-Resistant Densified Wood Composites
ACS Sustainable Chemistry & Engineering · 09.11.2026 · 14 (44) · 20288-20303
DOI: 10.1021/acssuschemeng.6c07162 ↗Kurz gefasst
Fachartikel in der Zeitschrift ACS Sustainable Chemistry & Engineering, online erschienen am 25.10.2026. Verfasst von Juya Zhu und 7 weiteren Autor:innen. Die Arbeit nennt 86 Literaturangaben. Gefördert von: National Basic Research Program of China (973 Program), National Natural Science Foundation of China (NSFC).
Abstract (Originalsprache)
Developing wood engineering materials that simultaneously satisfy flame retardancy and mechanical requirements remains a formidable challenge. Inspired by the formation of nacre and bone in natural biomineralization, this study proposes a biomimetic mineralization strategy based on interface engineering to overcome the inherent flammability and mechanical limitations inherited from the porous structure of natural wood. The in-situ mineralization on microfibril surfaces was facilitated by the hydroxyl-rich cellulose scaffold generated through delignification, which provided abundant interfacial sites for mineral nucleation and growth. Mg2+ was used to regulate the crystallization pathway of calcium carbonate. To establish an intimate interlocking for enhanced interfacial stress transfer, the hot-pressing densification process was employed to promote the deep compaction of the mineral phases and the cellulose skeleton. Consequently, the optimized sample with a Mg2+/Ca2+ molar ratio of 5:1 exhibited an LOI of 37.0%, the total heat release (THR) reached 21.46 MJ/m2, and the peak heat release rate (PHRR) suppressed to 133.94 kW/m2. Regarding mechanical performance, the flexural strength surged to 359.85 ± 10.93 MPa, representing approximately 4.6 times the flexural strength of natural wood, with the specific strength further elevated to 295.82 ± 8.99 MPa·cm3/g. Furthermore, the mineralized and hot-pressed composite exhibited a higher initial apparent water contact angle and improved dimensional stability under high-humidity conditions. Even under extreme humidity (95% RH), the optimized sample maintained a robust flexural strength of 210.39 ± 27.07 MPa, which is approximately three times that of wet natural wood. This study reveals the pivotal role of the Mg2+/Ca2+ molar ratio in balancing phase separation and atomic regulation, providing a novel pathway for the design of high-performance, fire-safe wood structural materials.
Förderung
- National Basic Research Program of China (973 Program)
- National Natural Science Foundation of China (NSFC)
Zitieren
APA
Zhu, J., Wang, Z., Zhang, Z., Zhang, G., Liu, X., Wang, Q., Chen, M., & Zhou, X. (2026). Biomimetic Mg-Regulated Mineralization of Aragonite Laths for High-Strength and Fire-Resistant Densified Wood Composites. ACS Sustainable Chemistry & Engineering, 14(44), 20288-20303. https://doi.org/10.1021/acssuschemeng.6c07162
Vancouver
Zhu J, Wang Z, Zhang Z, Zhang G, Liu X, Wang Q, et al. Biomimetic Mg-Regulated Mineralization of Aragonite Laths for High-Strength and Fire-Resistant Densified Wood Composites. ACS Sustainable Chemistry & Engineering. 2026;14(44):20288-20303. doi:10.1021/acssuschemeng.6c07162
BibTeX
@article{Zhu2026,
author = {Zhu, Juya and Wang, Zhe and Zhang, Zhongyu and Zhang, Guohang and Liu, Xiaohan and Wang, Qi and Chen, Minzhi and Zhou, Xiaoyan},
title = {Biomimetic Mg-Regulated Mineralization of Aragonite Laths for High-Strength and Fire-Resistant Densified Wood Composites},
journal = {ACS Sustainable Chemistry & Engineering},
year = {2026},
volume = {14},
number = {44},
pages = {20288--20303},
doi = {10.1021/acssuschemeng.6c07162}
}
EUVIMED