Improved Li+ Transport and Interfacial Stability in PEO-LiTFSI Solid Electrolytes via Al2O3 Ceramic Fillers at 20 °C
ACS Omega · 04.08.2026 · 11 (30) · 45104-45120
DOI: 10.1021/acsomega.6c03400 ↗Kurz gefasst
Fachartikel in der Zeitschrift ACS Omega, online erschienen am 17.07.2026. Verfasst von Mahdieh Hakimi und 4 weiteren Autor:innen. Beteiligte Einrichtung: Iberian Centre for Research in Energy Storage (CIIAE), Av. de la Universidad s/n, 10003 Cáceres, Extremadura, Spain. Die Arbeit nennt 78 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0). Gefördert von: Cofinanciado al 85% por la Uni??n Europea, Fondo Europeo de Desarrollo Regional, y la Junta de Extremadura, Autoridad de Gesti??n Ministerio de Hacienda.
Abstract (Originalsprache)
Incorporation of ceramic nanofillers (Al2O3, SiO2, TiO2) into PEO-based solid electrolytes is investigated to compare their effects on Li+ transport and address the low room-temperature conductivity of PEO by reducing polymer crystallinity and facilitating Li+ migration through the amorphous phase. Among the tested fillers, 5 wt % Al2O3 reduces membrane crystallinity by ≈ 11% and increases ionic conductivity by ≈1.8-fold. Comparative analysis suggests that Al2O3 stands out due to possible interactions with PEO ether oxygens, as supported by structural and spectroscopic analyses. These interactions generate interconnected Li+ transport pathways along polymer–filler interfaces, improving ionic conduction. Structural (XRD, FTIR, Raman) and thermal (TGA/DSC) analyses confirm an amorphous and thermally stable network. Electrochemical studies demonstrate that the Al2O3-containing membrane provides extended oxidation stability up to 5.22 V, with Li+ transference number and diffusion coefficient 2.58 and 8 times higher than those of the filler-free PEO-LiTFSI system, respectively. This membrane displays reduced overpotential and an almost 100% recovery ratio after current-step cycling, emphasizing superior interfacial compatibility. Stable Li plating/stripping for ≈780 h at 50 μA cm–2 further confirms suppression of lithium dendrite growth, achieving a cycling lifetime 5.5 times longer. These findings highlight the role of Al2O3 in promoting efficient low-temperature interfacial Li+ conduction, offering promising insights for the design of solid polymer electrolytes.
Autor:innen und Institutionen
- Iberian Centre for Research in Energy Storage (CIIAE), Av. de la Universidad s/n, 10003 Cáceres, Extremadura, Spain.
ORCID-Profile: Mahdieh Hakimi, Robert V Kamalov, V Vedavyas
Förderung
- Cofinanciado al 85% por la Uni??n Europea, Fondo Europeo de Desarrollo Regional, y la Junta de Extremadura
- Autoridad de Gesti??n Ministerio de Hacienda
Zitieren
APA
Hakimi, M., Kamalov, R. V., Vedavyas, V., Pérez, J. M., & Ortiz, M. G. (2026). Improved Li+ Transport and Interfacial Stability in PEO-LiTFSI Solid Electrolytes via Al2O3 Ceramic Fillers at 20 °C. ACS Omega, 11(30), 45104-45120. https://doi.org/10.1021/acsomega.6c03400
Vancouver
Hakimi M, Kamalov RV, Vedavyas V, Pérez JM, Ortiz MG. Improved Li+ Transport and Interfacial Stability in PEO-LiTFSI Solid Electrolytes via Al2O3 Ceramic Fillers at 20 °C. ACS Omega. 2026;11(30):45104-45120. doi:10.1021/acsomega.6c03400
BibTeX
@article{Hakimi2026,
author = {Hakimi, Mahdieh and Kamalov, Robert V and Vedavyas, V and Pérez, Juan M and Ortiz, Mariela G},
title = {Improved Li+ Transport and Interfacial Stability in PEO-LiTFSI Solid Electrolytes via Al2O3 Ceramic Fillers at 20 °C},
journal = {ACS Omega},
year = {2026},
volume = {11},
number = {30},
pages = {45104--45120},
doi = {10.1021/acsomega.6c03400}
}
EUVIMED