Highly Improved Shape Memory Properties of a PCL-Based Polyurethane via Polylactide Stereocomplexation

Zhiyou Xue, Jin Wang, Xin Li, Lingchen Mao, Sizhe Tao, Zihao Li, Ziqi Luo, Suyang Dai, Ni Jiang iD, Zhihua Gan, Zhenbo Ning iD

ACS Applied Materials & Interfaces · 2025-05-14 · 17 (19) · 28704-28715

DOI: 10.1021/acsami.5c04033 ↗

At a glance

Journal article in ACS Applied Materials & Interfaces, published online on 2025-05-02. Written by Zhiyou Xue and 10 co-authors. Institution: State Key Laboratory of Organic-Inorganic Composites, Beijing Laboratory of Biomedical Materials, College of Life Science and Technology, Beijing Uni…. Cited 14 times so far (Crossref); 38 references. Funded by: China Postdoctoral Science Foundation, Natural Science Foundation of Beijing Municipality, National Natural Science Foundation of China.

AbstractSubjectsBibliografiske oplysningerCiteRelated studies

Abstract (original language)

In shape memory polymers (SMPs) composed of semicrystalline polymers, their crystallization-melting process and the overall entropic elasticity of the material determine their shape memory behavior. In this work, cross-linked polyurethanes with polycaprolactone (PCL), poly(l-lactic acid) (PLLA), and poly(d-lactic acid) (PDLA) segments were designed, in which four-armed PCL served as the chemical cross-linking and polylactic acid (PLA) crystals acted as physical cross-linking. By adjusting the molecular weight of the four-armed PCL and the type of PLA crystals [homocrystals (HC) and stereocomplex (SC) crystals], the overall cross-linking degree of the material was controlled, and the crystallization behavior, mechanical properties, and shape memory behavior of the material were studied. The results indicated that both physical and chemical cross-linking significantly affect the mechanical properties and shape memory properties of materials. Moreover, polyurethane-contained SC exhibited a higher shape recovery ratio (Rr) and fixation ratio (Rf) than polyurethane-contained HC because SC provided higher entropy elasticity and promoted PCL crystallization. This study provides a method for synergistically enhancing Rf and Rr of SMPs, offering insights into the design of related materials.

Subjects

Author keywords

polycaprolactonepolylactic acidprogrammableshape memory polymersstereocomplex crystals

Authors and institutions

  • State Key Laboratory of Organic-Inorganic Composites, Beijing Laboratory of Biomedical Materials, College of Life Science and Technology, Beijing University of Chemical Technology, Beijing 100029, China.

ORCID profiles: Ni Jiang, Zhenbo Ning

Funding

  • China Postdoctoral Science Foundation
  • Natural Science Foundation of Beijing Municipality
  • National Natural Science Foundation of China

Cite

APA

Xue, Z., Wang, J., Li, X., Mao, L., Tao, S., Li, Z., Luo, Z., Dai, S., Jiang, N., Gan, Z., & Ning, Z. (2025). Highly Improved Shape Memory Properties of a PCL-Based Polyurethane via Polylactide Stereocomplexation. ACS Applied Materials & Interfaces, 17(19), 28704-28715. https://doi.org/10.1021/acsami.5c04033

Vancouver

Xue Z, Wang J, Li X, Mao L, Tao S, Li Z, et al. Highly Improved Shape Memory Properties of a PCL-Based Polyurethane via Polylactide Stereocomplexation. ACS Applied Materials & Interfaces. 2025;17(19):28704-28715. doi:10.1021/acsami.5c04033

BibTeX
@article{Xue2025,
  author = {Xue, Zhiyou and Wang, Jin and Li, Xin and Mao, Lingchen and Tao, Sizhe and Li, Zihao and Luo, Ziqi and Dai, Suyang and Jiang, Ni and Gan, Zhihua and Ning, Zhenbo},
  title = {Highly Improved Shape Memory Properties of a PCL-Based Polyurethane via Polylactide Stereocomplexation},
  journal = {ACS Applied Materials & Interfaces},
  year = {2025},
  volume = {17},
  number = {19},
  pages = {28704--28715},
  doi = {10.1021/acsami.5c04033}
}
Start for free →