EUVIMEDEUVIMED entdecken
Vergleichsstudie

Enamel wear and fatigue resistance of 3D printed resin compared with lithium disilicate

Pranit V Bora, Nathaniel C Lawson, Daniel A Givan, Celin Arce, Howard Roberts

The Journal of Prosthetic Dentistry · 2025-02 · 133 (2) · 523.e1-523.e9

DOI: 10.1016/j.prosdent.2024.10.024 ↗

Kurz gefasst

Vergleichsstudie in der Zeitschrift The Journal of Prosthetic Dentistry, 2025-02. Verfasst von Pranit V Bora und 4 weiteren Autor:innen. Beteiligte Einrichtung: Clinical Assistant Professor, Department of Clinic Essentials and Simulation, School of Dentistry, University of Detroit Mercy, Detroit, Mich. Hauptthemen laut MEDLINE: Dental Porcelain, Printing, Three-Dimensional, Dental Enamel, Crowns. Die Arbeit wurde bisher 12-mal zitiert (Crossref) und nennt 33 Literaturangaben. Gefördert von: American Academy of Fixed Prosthodontics.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

STATEMENT OF PROBLEM: The effect of 3-dimensional (3D) printed crown materials with lower flexural strength but higher ductility than lithium disilicate on enamel wear and fatigue resistance is unknown. PURPOSE: The purpose of this in vitro study was to compare the enamel wear and fatigue resistance of a 50% filled 3D printed crown material with lithium disilicate. MATERIAL AND METHODS: Disks of a 3D printed crown material (Ceramic Crown; SprintRay Inc) and lithium disilicate (IPS e.max CAD; Ivoclar AG) (n=8) were tested for wear in a custom Alabama wear testing device which applied a 20-N load and 2-mm horizontal slide. The test was run for 400 000 cycles at 1 Hz in a 33% glycerin solution. Cusps of extracted human molars were used as the antagonists. The volumetric wear of the restorative material and enamel antagonists were measured every 100 000 cycles using a profilometer. Worn specimens were examined with a scanning electron microscope. Human molars were prepared for occlusal onlay preparations, and 1.2-mm 3D printed (Ceramic Crown) or lithium disilicate (IPS e.max CAD) restorations (n=10) were bonded to the teeth with resin cement. Restorations were subjected to 2 million cycles of fatigue loading (50 N, 1 Hz) in water against a Ø7.8-mm steel ball. Restorations were monitored for cracks every 100 000 cycles with transillumination and every1 million cycles with microcomputed tomography (µCT). After fatigue, specimens were fractured in a load-to-failure test. Fractured specimens were examined with µCT. Statistical analyses were performed with 2-way mixed ANOVAs and a t test (α=.05). RESULTS: The wear and opposing enamel wear of lithium disilicate was greater than the 3D printed material at every interval of cycles tested (P

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

Dental PorcelainPrinting, Three-DimensionalDental EnamelCrownsTooth WearDental Restoration WearDental MaterialsHumansMaterials TestingIn Vitro TechniquesDental Stress AnalysisMicroscopy, Electron, Scanning

Substanzen

lithia disilicateDental PorcelainDental Materials

Autor:innen und Institutionen

  • Clinical Assistant Professor, Department of Clinic Essentials and Simulation, School of Dentistry, University of Detroit Mercy, Detroit, Mich.
  • Associate Professor, Department of Clinical and Community Sciences, School of Dentistry, University of Alabama at Birmingham, Birmingham, Ala. Electronic address: nlawson@uab.edu.
  • Professor and Clinical Dean, Department of Restorative Sciences, School of Dentistry, University of Alabama at Birmingham, Birmingham, Ala.
  • Assistant Professor, Department of Oral Health Practice, University of Kentucky School of Dentistry, Lexington, KY.
  • Associate Professor, Department of Oral Health Practice, University of Kentucky School of Dentistry, Lexington, KY.

Förderung

  • American Academy of Fixed Prosthodontics

Zitieren

APA

Bora, P. V., Lawson, N. C., Givan, D. A., Arce, C., & Roberts, H. (2025). Enamel wear and fatigue resistance of 3D printed resin compared with lithium disilicate. The Journal of Prosthetic Dentistry, 133(2), 523.e1-523.e9. https://doi.org/10.1016/j.prosdent.2024.10.024

Vancouver

Bora PV, Lawson NC, Givan DA, Arce C, Roberts H. Enamel wear and fatigue resistance of 3D printed resin compared with lithium disilicate. The Journal of Prosthetic Dentistry. 2025;133(2):523.e1-523.e9. doi:10.1016/j.prosdent.2024.10.024

BibTeX
@article{Bora2025,
  author = {Bora, Pranit V and Lawson, Nathaniel C and Givan, Daniel A and Arce, Celin and Roberts, Howard},
  title = {Enamel wear and fatigue resistance of 3D printed resin compared with lithium disilicate},
  journal = {The Journal of Prosthetic Dentistry},
  year = {2025},
  volume = {133},
  number = {2},
  pages = {523.e1--523.e9},
  doi = {10.1016/j.prosdent.2024.10.024}
}
Kostenlos starten →