Fracture Resistance of Heat-treated NiTi Instruments by the Load of Mechanical Preparation According to Tooth Type and Canal Number
Journal of Endodontics · 2026
DOI: 10.1016/j.joen.2026.02.005 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Endodontics, 2026. Verfasst von Badria AlAli und 6 weiteren Autor:innen. Beteiligte Einrichtung: Endodontic Department, Hamdan Bin Mohammed College of Dental Medicine, Mohammed Bin Rashid University of Medicine and Health Sciences, Dubai Health, …. Hauptthemen laut MEDLINE: Nickel, Titanium, Root Canal Preparation, Dental Alloys. Die Arbeit nennt 28 Literaturangaben.
Abstract (Originalsprache)
INTRODUCTION: This study aimed to evaluate the impact of mechanical loading, induced by preparing anatomically standardized premolar and molar canal models, on the cyclic fatigue and torsional fracture resistance of heat-treated nickel-titanium (NiTi) rotary instruments. METHODS: Sixty NiTi instruments (Race Evo) were randomly assigned to 3 groups (n = 20): unused controls (N0), instruments used to prepare 2 canals in premolar models (P2), and 4 canals in molar models (M4). Cyclic fatigue testing was performed in dynamic mode with a 4 mm axial pecking motion at 37 ± 1 °C. Time to fracture and the number of cycles to fracture were recorded; the lengths of fractured fragments were measured using a digital caliper. Torsional resistance was assessed by fixing the apical 3 mm and rotating the shaft until fracture. Maximum torsional load and angle of rotation were recorded. Fractured surfaces were examined using scanning electron microscopy, and phase transformation behavior was assessed via differential scanning calorimetry. Data were analyzed using one-way analysis of variance and Tukey's post hoc test at a 95% significance level. RESULTS: P2 and M4 groups showed significantly higher cyclic fatigue resistance than N0 (P < .001), with no difference between P2 and M4. Torsional resistance parameters were significantly reduced in P2 and M4 compared to N0 (P < .05). Scanning electron microscopy revealed distinct fracture morphologies; differential scanning calorimetry showed consistent phase transformation behavior. CONCLUSION: Within the limitations of this study, standardized simulated procedural loading paradoxically increased the cyclic fatigue resistance of heat-treated NiTi instruments, while simultaneously producing a moderate reduction in torsional strength.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Endodontic Department, Hamdan Bin Mohammed College of Dental Medicine, Mohammed Bin Rashid University of Medicine and Health Sciences, Dubai Health, Dubai, United Arab Emirates.
- Biostatistics Department, Hamdan Bin Mohammed College of Dental Medicine, Mohammed Bin Rashid University of Medicine and Health Sciences, Dubai Health, Dubai, United Arab Emirates.
- Department of Conservative Dentistry, School of Dentistry, Dental Research Institute, Dental and Life Science Institute, Pusan National University, Yangsan, Republic of Korea. Electronic address: golddent@pusan.ac.kr.
- Endodontic Department, Hamdan Bin Mohammed College of Dental Medicine, Mohammed Bin Rashid University of Medicine and Health Sciences, Dubai Health, Dubai, United Arab Emirates. Electronic address: rashid.elabed@dubaihe…
Zitieren
APA
AlAli, B., Atmeh, A., Jamal, M., Ahmad, F., Khamis, A. H., Kim, H. C., & El Abed, R. (2026). Fracture Resistance of Heat-treated NiTi Instruments by the Load of Mechanical Preparation According to Tooth Type and Canal Number. Journal of Endodontics. https://doi.org/10.1016/j.joen.2026.02.005
Vancouver
AlAli B, Atmeh A, Jamal M, Ahmad F, Khamis AH, Kim HC, et al. Fracture Resistance of Heat-treated NiTi Instruments by the Load of Mechanical Preparation According to Tooth Type and Canal Number. Journal of Endodontics. 2026. doi:10.1016/j.joen.2026.02.005
BibTeX
@article{AlAli2026,
author = {AlAli, Badria and Atmeh, Amre and Jamal, Mohamed and Ahmad, Fatemeh and Khamis, Amar H and Kim, Hyeon-Cheol and El Abed, Rashid},
title = {Fracture Resistance of Heat-treated NiTi Instruments by the Load of Mechanical Preparation According to Tooth Type and Canal Number},
journal = {Journal of Endodontics},
year = {2026},
doi = {10.1016/j.joen.2026.02.005}
}
EUVIMED