Abstract (Originalsprache)

AIM or PURPOSE This study aimed to compare the shear bond strength (SBS) of Biodentine and MTA Angelus (MTA) to a novel self-cure bulk-fill composite (Stela Automix) using two different application techniques. MATERIALS and METHODS Thirty-six acrylic blocks with cylindrical cavities were prepared and randomly divided into four experimental groups: Biodentine/Bond, Biodentine/Primer, MTA/Bond, and MTA/Primer. After the MTA and Biodentine were placed and allowed to set. For the primer groups, only Stela Primer was applied for 5 seconds. For the bond groups, the 3M ESPE Scotchbond Universal Plus was applied and light-cured for 10 seconds. Subsequently, Stela Automix was injected and polymerized. SBS values were measured in Newtons using a universal testing device and converted to megapascals. Data were statistically analyzed using two-way ANOVA, Tukey, and Bonferroni tests. Failure mode distributions were evaluated using the Chi-square test (p < 0.05). RESULTS MTA groups exhibited significantly higher SBS values compared to Biodentine groups. The application techniques (Bond vs. Primer) did not have a significant independent effect on SBS values (p = 0.916). While the interaction between material type and technique was not statistically significant (p = 0.070), post-hoc analyses revealed a significant difference specifically between the Biodentine/Primer and MTA/Primer groups (p = 0.002). Failure mode distributions showed statistically significant differences among the groups (p < 0.05). CONCLUSIONS MTA showed significantly higher SBS to the self-cure bulk-fill composite than Biodentine. The use of primer or bonding did not significantly influence the SBS values.

Zitieren

APA

Ogurlu, İ. D., & Oncu, A. (2026). Shear bond strength of MTA and Biodentine to STELA Automix. International Dental Journal, 76, 110451. https://doi.org/10.1016/j.identj.2026.110451

Vancouver

Ogurlu İD, Oncu A. Shear bond strength of MTA and Biodentine to STELA Automix. International Dental Journal. 2026;76:110451. doi:10.1016/j.identj.2026.110451

BibTeX
@article{Ogurlu2026,
  author = {Ogurlu, İdil Dilan and Oncu, Aysenur},
  title = {Shear bond strength of MTA and Biodentine to STELA Automix},
  journal = {International Dental Journal},
  year = {2026},
  volume = {76},
  pages = {110451},
  doi = {10.1016/j.identj.2026.110451}
}
Kostenlos starten →