Fracture strength of three-unit zirconia fixed partial dentures fabricated with different manufacturing protocols: An in vitro study

Andreas Hönigl, Alexander Pfanner, Lars Stucki, Sebastian Fitzek, Rüdiger Junker, Maximilian Nothaft

Digital Dentistry Journal · 2026-12 · 4 (1) · 100111

DOI: 10.1016/j.ddj.2026.100111 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Digital Dentistry Journal, 2026-12. Verfasst von Andreas Hönigl und 5 weiteren Autor:innen. Die Arbeit nennt 29 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

(230 words): Purpose This in vitro study evaluated the fracture strength of three-unit fixed dental prostheses made from zirconia by comparing ceramic-veneered zirconia bridges to monolithic milled zirconia bridges. To examine the impact of the manufacturing process involved in veneered bridges, zirconia cores were tested before and after the firing process. Materials and Methods A load-to-fracture test was conducted using a modified model design by Junker et al. 2024. Four test groups were formed, each containing 10 three-unit bridges: zirconia core (A), fired zirconia core (B), veneered zirconia core (C), and fully anatomical monolithic milled zirconia (D). For our analysis, IPS e.max ZirCAD Prime was used. The model used 3-unit bridges spanning from tooth 35 to 37, which were adhesively bonded to the artificial teeth using Multilink (Ivoclar). To standardize the luting process, a force of 20 N was applied for 8 minutes. After cementation, the load-to-fracture test was performed by applying forces until fracture. Statistical analysis included Welch one-way ANOVA with Games-Howell post-hoc comparisons (Holm-adjusted p-values).

Results

The study found that fully anatomical monolithic milled bridges had a mean fracture strength of 2838.3 N, significantly higher than veneered bridges, which averaged 1007.6 N (Holm-adjusted p = 0.001). Firing the frameworks reduced the mean fracture strength from 1639.7 N to 1157.1 N (Holm-adjusted p = 0.015).

Conclusion

Within the limitations of this study, monolithic zirconia bridges exhibit significantly greater fracture strength compared to veneered bridges, while firing seems to weaken zirconia cores.

Zitieren

APA

Hönigl, A., Pfanner, A., Stucki, L., Fitzek, S., Junker, R., & Nothaft, M. (2026). Fracture strength of three-unit zirconia fixed partial dentures fabricated with different manufacturing protocols: An in vitro study. Digital Dentistry Journal, 4(1), 100111. https://doi.org/10.1016/j.ddj.2026.100111

Vancouver

Hönigl A, Pfanner A, Stucki L, Fitzek S, Junker R, Nothaft M. Fracture strength of three-unit zirconia fixed partial dentures fabricated with different manufacturing protocols: An in vitro study. Digital Dentistry Journal. 2026;4(1):100111. doi:10.1016/j.ddj.2026.100111

BibTeX
@article{Hnigl2026,
  author = {Hönigl, Andreas and Pfanner, Alexander and Stucki, Lars and Fitzek, Sebastian and Junker, Rüdiger and Nothaft, Maximilian},
  title = {Fracture strength of three-unit zirconia fixed partial dentures fabricated with different manufacturing protocols: An in vitro study},
  journal = {Digital Dentistry Journal},
  year = {2026},
  volume = {4},
  number = {1},
  pages = {100111},
  doi = {10.1016/j.ddj.2026.100111}
}
Kostenlos starten →