EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Brazing of Sn78Cu22 on aluminum substrates observed via in-situ experiments in a large-chamber SEM

Shohreh Khatami, Joachim Mayer, Anke Aretz, Bei Zhou, Markus Apel

Discover Mechanical Engineering · 12.03.2026 · 5 (1)

DOI: 10.1007/s44245-026-00209-8 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Discover Mechanical Engineering, online erschienen am 12.03.2026. Verfasst von Shohreh Khatami und 4 weiteren Autor:innen. Die Arbeit nennt 21 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: RWTH Aachen University.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

In situ brazing is a powerful method for understanding dynamic material behavior during joining process, enabling real-time observation of melting, wetting, and interfacial reactions. The present study investigates the influence of aluminum alloy chemical composition on wetting behavior and interfacial phase formation during soldering with a Sn78Cu22 alloy. The experiments were performed inside a large-chamber scanning electron microscope (LC-SEM) to monitor heat-induced deformation, melting, melt propagation, elemental segregation, and solidification. Microstructural and compositional analyses were carried out using SEM/EDX and TEM, supported by thermodynamic calculations using Thermo-Calc. Despite the low melting point of Sn78Cu22, solder reactions could only be initiated at significantly higher temperatures, namely 466 °C for EN AC-42,100, 500 °C for EN AW-5083, and 600 °C for EN AW-3003, due to the presence of stable surface oxide films. The Si-rich EN AC-42,100 alloy exhibited early filler deformation and formation of Al–Cu and Cu–Sn intermetallic compounds, namely Cu 6 Sn 5 , Cu 2 Sn, while Sn wetting was limited by a Si diffusion barrier. In contrast, the EN AW-5083 and EN AW-3003 alloys showed delayed wetting caused by MgO and MgAl 2 O 4 oxide layers, respectively. For EN AW-5083, Mg reacted with Sn to form Mg 2 Sn within the filler and at the interface, accompanied by Al–Cu formation. For EN AW-3003, Al–Cu interdiffusion led to the formation of Cu-rich Al 4 Cu 9 -type intermetallics with shallow Sn penetration. These results demonstrate that aluminum alloy chemistry critically governs wetting kinetics and interfacial reactions during soldering with Sn78Cu22.

Förderung

  • RWTH Aachen University

Zitieren

APA

Khatami, S., Mayer, J., Aretz, A., Zhou, B., & Apel, M. (2026). Brazing of Sn78Cu22 on aluminum substrates observed via in-situ experiments in a large-chamber SEM. Discover Mechanical Engineering, 5(1). https://doi.org/10.1007/s44245-026-00209-8

Vancouver

Khatami S, Mayer J, Aretz A, Zhou B, Apel M. Brazing of Sn78Cu22 on aluminum substrates observed via in-situ experiments in a large-chamber SEM. Discover Mechanical Engineering. 2026;5(1). doi:10.1007/s44245-026-00209-8

BibTeX
@article{Khatami2026,
  author = {Khatami, Shohreh and Mayer, Joachim and Aretz, Anke and Zhou, Bei and Apel, Markus},
  title = {Brazing of Sn78Cu22 on aluminum substrates observed via in-situ experiments in a large-chamber SEM},
  journal = {Discover Mechanical Engineering},
  year = {2026},
  volume = {5},
  number = {1},
  doi = {10.1007/s44245-026-00209-8}
}
Kostenlos starten →