Comparison of Static and Dynamic in Vitro Degradation of a Biodegradable Magnesium Implant Screw

Minna Siekkinen, Emil Vainio, Terhi J. Heino, Pekka Vallittu, Leena Hupa

Biomedical Materials & Devices · 10.11.2026

DOI: 10.1007/s44174-026-00800-3 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Biomedical Materials & Devices, online erschienen am 10.11.2026. Verfasst von Minna Siekkinen und 4 weiteren Autor:innen. Die Arbeit nennt 36 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Åbo Akademi University.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Degradation of biodegradable metals and precipitation of apatite on their surfaces are commonly studied in vitro under static immersion conditions. Such static environments do not accurately replicate the dynamic conditions in vivo. This study aimed to develop an in vitro setup that introduces controlled fluid flow to better represent transport conditions than conventional static immersion experiments. Magnesium alloy screws were immersed in Hank’s Balanced Salt Solution (HBSS) or Simulated Body Fluid (SBF) either directly or after fixation in closed-cell or open-cell porous synthetic bone models. Screws were also studied in a dynamic flow-through system in which the solution flowed along the screw surface. The initial burst release of magnesium ions and the accompanying increase in pH demonstrated that fluid flow significantly affects the degradation behavior of magnesium screws. SBF accelerated degradation compared with HBSS in all experimental configurations. Dynamic flow conditions revealed an initial burst release of magnesium ions followed by stabilization of both magnesium concentration and pH. For mechanistic in vitro studies, HBSS may be advantageous because the slower degradation rate allows the underlying processes to be followed over longer periods. In contrast, SBF may be advantageous when shorter experimental durations are desired. Surface analyses further revealed the formation of magnesium-containing corrosion products and calcium- and phosphorus-containing precipitates. Overall, the findings demonstrate that both solution composition and fluid flow strongly influence the degradation behavior of biodegradable magnesium implants. Dynamic testing conditions provide valuable information not obtainable from conventional static immersion experiments and should, therefore, be considered when evaluating biodegradable magnesium implants in vitro.

Förderung

  • Åbo Akademi University

Zitieren

APA

Siekkinen, M., Vainio, E., Heino, T. J., Vallittu, P., & Hupa, L. (2026). Comparison of Static and Dynamic in Vitro Degradation of a Biodegradable Magnesium Implant Screw. Biomedical Materials & Devices. https://doi.org/10.1007/s44174-026-00800-3

Vancouver

Siekkinen M, Vainio E, Heino TJ, Vallittu P, Hupa L. Comparison of Static and Dynamic in Vitro Degradation of a Biodegradable Magnesium Implant Screw. Biomedical Materials & Devices. 2026. doi:10.1007/s44174-026-00800-3

BibTeX
@article{Siekkinen2026,
  author = {Siekkinen, Minna and Vainio, Emil and Heino, Terhi J. and Vallittu, Pekka and Hupa, Leena},
  title = {Comparison of Static and Dynamic in Vitro Degradation of a Biodegradable Magnesium Implant Screw},
  journal = {Biomedical Materials & Devices},
  year = {2026},
  doi = {10.1007/s44174-026-00800-3}
}
Kostenlos starten →