Microstructure and tensile mechanical behavior of In alloyed Sn-Bi solder

Hongbo Lu, Xiaobing Luo, Chen Liu, Yuanwei Jia, Ahmed M. Fallatah, Gaber A. M. Mersal, Jinzhi Peng, Xin Zhang, Abdulraheem S. A. Almalki, Zhiqi Yu, Hao Yang, Xiaojing Wang und 3 weitere

Journal of Materials Science: Materials in Electronics · 2025-08 · 36 (24)

DOI: 10.1007/s10854-025-15519-y ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Materials Science: Materials in Electronics, online erschienen am 21.08.2025. Verfasst von Hongbo Lu und 14 weiteren Autor:innen. Die Arbeit wurde bisher 6-mal zitiert (Crossref) und nennt 62 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Currently, Sn–Pb alloy remains the primary solder used for interconnecting solar cell arrays. Amidst the growing pressure from environmental protection, the need for lead-free, low-temperature alloys in photovoltaics has emerged as a significant concern. This article explores the impact of x In on the melting properties, microstructure, and mechanical properties of Sn-30Bi ( x = 0, 0.5, 1, 2, 4, 6, 8, 10 wt.%, mass fraction) alloy, utilizing differential scanning calorimetry, scanning electron microscopy, X-ray diffraction, and tensile testing. The findings reveal that as the In content increases, the solidus and liquidus temperatures of the Sn-30Bi alloy decline. The microstructure of the alloy, post the addition of 0.5, 1, 2, and 4 wt.% In, comprises β-Sn dendrites, Sn-Bi eutectic, and Bi particles. The incorporation of In homogenizes the distribution of Bi precipitates, leading to a complex eutectic mixture. Alloys containing 6, 8, and 10 wt.% In exhibit β-phase, BiIn-phase, and Bi-phase structures. At room temperature, In-doping enhances the tensile strength of the alloy. Notably, the ultimate tensile strength (UTS) of the 4 wt.% In doped alloy experiences the most significant increase, reaching 87 MPa, while the elongation rate peaks at 1 wt.% In doped alloy, attaining 29.8%. When tensile tests were carried out at high temperatures (60, 80, 100, and 120 °C), the maximum elongation of the alloy at 120 °C reached 150% after adding 1% In. This research finding holds significant importance for enhancing the mechanical properties of photovoltaic solder strip.

Zitieren

APA

Lu, H., Luo, X., Liu, C., Jia, Y., Fallatah, A. M., Mersal, G. A. M., Peng, J., Zhang, X., Almalki, A. S. A., Yu, Z., Yang, H., Wang, X., Guo, Z., Ren, J., & Algadi, H. (2025). Microstructure and tensile mechanical behavior of In alloyed Sn-Bi solder. Journal of Materials Science: Materials in Electronics, 36(24). https://doi.org/10.1007/s10854-025-15519-y

Vancouver

Lu H, Luo X, Liu C, Jia Y, Fallatah AM, Mersal GAM, et al. Microstructure and tensile mechanical behavior of In alloyed Sn-Bi solder. Journal of Materials Science: Materials in Electronics. 2025;36(24). doi:10.1007/s10854-025-15519-y

BibTeX
@article{Lu2025,
  author = {Lu, Hongbo and Luo, Xiaobing and Liu, Chen and Jia, Yuanwei and Fallatah, Ahmed M. and Mersal, Gaber A. M. and Peng, Jinzhi and Zhang, Xin and Almalki, Abdulraheem S. A. and Yu, Zhiqi and Yang, Hao and Wang, Xiaojing and Guo, Zhanhu and Ren, Juanna and Algadi, Hassan},
  title = {Microstructure and tensile mechanical behavior of In alloyed Sn-Bi solder},
  journal = {Journal of Materials Science: Materials in Electronics},
  year = {2025},
  volume = {36},
  number = {24},
  doi = {10.1007/s10854-025-15519-y}
}
Kostenlos starten →