In-vitro evaluation of fracture resistance of teeth restored with different high-viscosity glass ionomer restorative materials and bulk-fill composite resins
Clinical Oral Investigations · 2024
DOI: 10.1007/s00784-024-05745-9 ↗Kurz gefasst
Fachartikel in der Zeitschrift Clinical Oral Investigations, 2024. Verfasst von Merve Nezir und 1 weiteren Autor:innen. Beteiligte Einrichtung: Department of Restorative Dentistry, Faculty of Dentistry, Gazi University, Bişkek St. 1.St. Number:8, Çankaya, Ankara, 06490, Turkey. mervenezir@gaz…. Hauptthemen laut MEDLINE: Composite Resins, Dental Restoration, Permanent, Glass Ionomer Cements, Materials Testing. Die Arbeit wurde bisher 5-mal zitiert (Crossref) und nennt 46 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Gazi University.
Abstract (Originalsprache)
Objectives
This study aimed to evaluate the effect of restorations made with a glass-hybrid restorative system (GHRS), a high-viscosity glass ionomer restorative material (HVGIC), a high-viscosity bulk-fill composite resin (HVB), a flowable bulk-fill composite resin (FB), and a nanohybrid composite resin (NH), which are commonly preferred in clinical applications on the fracture resistance of teeth in-vitro . Materials and methods One hundred intact human premolar teeth were included in the study. The teeth were randomly divided into ten groups ( n = 10). No treatment was applied to the teeth in Control group. Class II cavities were prepared on the mesial surfaces of the remaining ninety teeth in other groups. For restoration of the teeth, a GHRS, a HVGIC, a HVB, a FB, and a NH were used. Additionally, in four groups, teeth were restored using NH, GHRS, and HVGIC with open and closed-sandwich techniques. After 24 h, fracture resistance testing was performed. One-way ANOVA and Tukey HDS tests were used for statistical analysis of the data.
Results
The fracture resistance values of Control group were statistically significantly higher than those of GHRS, HVGIC, FB, NH, HVGIC-CS, GHRS-OS, and HVGIC-OS groups( p < 0.05). There was no statistically significant difference observed between the fracture resistance values of Control, HVB, and GHRS-CS groups ( p > 0.05).
Conclusion
It can be concluded that the use of HVB and the application of GHRS with a closed-sandwich technique may have a positive effect on the fracture resistance of teeth in the restoration of wide Class II cavities. Clinical relevance The use of high-viscosity bulk-fill composite resin and the application of glass-hybrid restorative system with the closed-sandwich technique in the restoration of teeth with wide Class II cavities could increase the fracture resistance of the teeth.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Department of Restorative Dentistry, Faculty of Dentistry, Gazi University, Bişkek St. 1.St. Number:8, Çankaya, Ankara, 06490, Turkey. mervenezir@gazi.edu.tr.
- Department of Restorative Dentistry, Faculty of Dentistry, Gazi University, Bişkek St. 1.St. Number:8, Çankaya, Ankara, 06490, Turkey.
ORCID-Profile: Merve Nezir, Suat Ozcan
Förderung
- Gazi University
Zitieren
APA
Nezir, M., & Ozcan, S. (2024). In-vitro evaluation of fracture resistance of teeth restored with different high-viscosity glass ionomer restorative materials and bulk-fill composite resins. Clinical Oral Investigations. https://doi.org/10.1007/s00784-024-05745-9
Vancouver
Nezir M, Ozcan S. In-vitro evaluation of fracture resistance of teeth restored with different high-viscosity glass ionomer restorative materials and bulk-fill composite resins. Clinical Oral Investigations. 2024. doi:10.1007/s00784-024-05745-9
BibTeX
@article{Nezir2024,
author = {Nezir, Merve and Ozcan, Suat},
title = {In-vitro evaluation of fracture resistance of teeth restored with different high-viscosity glass ionomer restorative materials and bulk-fill composite resins},
journal = {Clinical Oral Investigations},
year = {2024},
doi = {10.1007/s00784-024-05745-9}
}
EUVIMED