Structural evolution of layered oxide cathodes for spent Li–ion batteries: Degradation mechanism and repair strategy

Shan Jin, Jianquan Liang, Deying Mu, Tianning Lin, Yuyang Tian, Jian Zhang, Yue Wang, Meng Chen, Qingmo Shi, Changsong Dai

SusMat · 2023-06 · 3 (3) · 362-378

DOI: 10.1002/sus2.126 ↗

At a glance

Journal article in SusMat, published online on 2023-04-10. Written by Shan Jin and 9 co-authors. Cited 57 times so far (Crossref); 69 references. The full text is freely available (open access, CC BY 4.0). Funded by: National Natural Science Foundation of China, Natural Science Foundation of Heilongjiang Province.

AbstractBibliografiske oplysningerCiteRelated studies

Abstract (original language)

Sustainable development has long been recognized as one of the most critical issues in today's energy and environment‐conscious society. It has never been more urgent to recycle and reuse the end‐of‐life cathode materials. Here, this work systematically investigates the structure‐critical degradation mechanism of polycrystalline LiNi x Co y Mn 1− x − y O 2 (NCM), combining experimental characterization and DFT simulations. Targeting the key degradation factors, a synergistic repair strategy based on deep mechanochemical activation and heat treatment was successfully proposed to direct regenerate the degraded NCM material. Studies indicate the induction and promotion of synergistic repair technique on the reconstruction of particle morphology, the recovery of the chemical composition and crystal structure, and the favorable transformation of the impurities phase in the failed materials. In particular, the synergistic repair process induces a gradient distribution of LiF and further enables partial fluorine doping into the NCM surface, forming abundant oxygen vacancies and increasing the content of highly reactive Ni 2+ . Benefiting from the comprehensive treatment for the multi‐scale and multi‐form degradation behaviors, the repaired material exhibits a capacity of 176.8 mA h g −1 at 0.1 C, which is comparable to the corresponding commercial material (172.8 mA h g −1 ). The satisfactory capacity of the recovered cathode proves that it is an effective direct renovating strategy.

Funding

  • National Natural Science Foundation of China
  • Natural Science Foundation of Heilongjiang Province

Cite

APA

Jin, S., Liang, J., Mu, D., Lin, T., Tian, Y., Zhang, J., Wang, Y., Chen, M., Shi, Q., & Dai, C. (2023). Structural evolution of layered oxide cathodes for spent Li–ion batteries: Degradation mechanism and repair strategy. SusMat, 3(3), 362-378. https://doi.org/10.1002/sus2.126

Vancouver

Jin S, Liang J, Mu D, Lin T, Tian Y, Zhang J, et al. Structural evolution of layered oxide cathodes for spent Li–ion batteries: Degradation mechanism and repair strategy. SusMat. 2023;3(3):362-378. doi:10.1002/sus2.126

BibTeX
@article{Jin2023,
  author = {Jin, Shan and Liang, Jianquan and Mu, Deying and Lin, Tianning and Tian, Yuyang and Zhang, Jian and Wang, Yue and Chen, Meng and Shi, Qingmo and Dai, Changsong},
  title = {Structural evolution of layered oxide cathodes for spent Li–ion batteries: Degradation mechanism and repair strategy},
  journal = {SusMat},
  year = {2023},
  volume = {3},
  number = {3},
  pages = {362--378},
  doi = {10.1002/sus2.126}
}
Start for free →