Behavior and design of concrete‐filled steel stub columns incorporating sandstone quarry waste aggregate
Structural Concrete · 19.11.2026
DOI: 10.1002/suco.70887 ↗Kurz gefasst
Fachartikel in der Zeitschrift Structural Concrete, online erschienen am 19.11.2026. Verfasst von Yengkhom Tarun Singh und 1 weiteren Autor:innen. Die Arbeit nennt 79 Literaturangaben.
Abstract (Originalsprache)
Rapid depletion of natural aggregates and growing accumulation of quarry waste have intensified the need for structurally viable, waste‐derived construction materials. Sandstone quarrying and processing in Rajasthan (India), account for over 90% of national production and generate waste fractions of up to 55%, representing a largely untapped resource for sustainable aggregate substitution. This study presents the first experimental investigation into sandstone‐waste aggregate concrete‐filled steel tube (SWACFST) stub columns, evaluating natural coarse aggregate replacement with crushed sandstone debris at 0%–100% under two water‐to‐cement ratios ( w / c = 0.45 and 0.38). The program comprised material characterization, compressive strength evaluation of concrete cubes, and axial compression testing of 16 SWACFST stub columns. At 100% replacement, the 28‐day cube compressive strength decreased by 15.1% and 8.4% for w / c = 0.45 and 0.38, respectively, primarily due to aggregate crushing rather than cementitious matrix failure. However, the corresponding reduction in the axial capacity of the CFST stub columns remained comparatively limited relative to the 0% replacement specimens. The concrete‐filled specimens also exhibited axial capacities 200%–90% and 167%–76% higher than the corresponding hollow steel tubes for w / c = 0.45 and 0.38, respectively. All specimens failed by outward local buckling accompanied by infill concrete crushing. Reliability analysis against six design models (EN 1994‐1‐1, AISC 360, Han, Wang et al., W. Wang et al., and Achuthan et al.) yielded reliability indices of 1.31–2.14, indicating that existing formulations provide varying levels of conservatism and should be applied with caution. Ultimately, these findings demonstrate that SWACFST columns offer a structurally robust, high‐performance composite member. By effectively repurposing abundant quarry debris, this application not only mitigates the depletion of natural aggregates but also provides a sustainable, circular‐economy solution for modern urban infrastructure.
Zitieren
APA
Singh, Y. T., & Singh, T. G. (2026). Behavior and design of concrete‐filled steel stub columns incorporating sandstone quarry waste aggregate. Structural Concrete. https://doi.org/10.1002/suco.70887
Vancouver
Singh YT, Singh TG. Behavior and design of concrete‐filled steel stub columns incorporating sandstone quarry waste aggregate. Structural Concrete. 2026. doi:10.1002/suco.70887
BibTeX
@article{Singh2026,
author = {Singh, Yengkhom Tarun and Singh, Tekcham Gishan},
title = {Behavior and design of concrete‐filled steel stub columns incorporating sandstone quarry waste aggregate},
journal = {Structural Concrete},
year = {2026},
doi = {10.1002/suco.70887}
}
EUVIMED