EUVIMEDObjevte EUVIMED
Crossref

Fracture Behavior of Active PLA Food Packaging Films: EWF and SEM Analysis

Neda Tajari, Hassan Sadrnia, Fereshteh Hosseini, Jasim Ahmed

Polymer Engineering & Science · 2026-08 · 66 (8) · 5783-5793

DOI: 10.1002/pen.70609 ↗

At a glance

Journal article in Polymer Engineering & Science, published online on 2026-05-26. Written by Neda Tajari and 3 co-authors. 44 references. Funded by: College of Agriculture, Ferdowsi University of Mashhad.

AbstraktBibliografické údajeCiteRelated studies

Abstract (original language)

Polylactic acid (PLA)‐based biodegradable polymers have potential for active packaging in the food industry. Extensive research has been conducted on the fabrication of PLA films to overcome their brittleness and improve their performance. However, studies on the fracture behavior of these films are very limited. Given the importance of fracture behavior, this study was designed to investigate the fracture behavior of PLA composite films by blending them with neroli and thyme essential oils, as well as spherical and rod‐shaped zinc oxide nanoparticles. The fracture behavior was analyzed using SEM images along with ImageJ software, following the essential work of fracture technique. Results from SEM revealed that the films exhibited ductile fracture characterized by cavity formation, followed by crazing and crack propagation. The shape of the cavities was found to be less circular before fracture, which transformed to more rounded after fracture with distinct visibility. The percentage of porosity increased after fracture, indicating the development and coalescence of more cavities when the material underwent deformation and failure. The specific essential work of fracture ( w e ) for the film containing rod‐shaped nanoparticles, which was one of the two control films for the active films, had the highest value (16.66 kJ/m 2 ), indicating that this film absorbed more energy in the elastic region compared to other films. The shape factor multiplied by the specific nonessential work of fracture ( βw p ) for the film containing spherical‐shaped nanoparticles, which was one of the two control films for the active films, had the highest value (6.08 MJ/m 3 ).

Funding

  • College of Agriculture, Ferdowsi University of Mashhad

Cite

APA

Tajari, N., Sadrnia, H., Hosseini, F., & Ahmed, J. (2026). Fracture Behavior of Active PLA Food Packaging Films: EWF and SEM Analysis. Polymer Engineering & Science, 66(8), 5783-5793. https://doi.org/10.1002/pen.70609

Vancouver

Tajari N, Sadrnia H, Hosseini F, Ahmed J. Fracture Behavior of Active PLA Food Packaging Films: EWF and SEM Analysis. Polymer Engineering & Science. 2026;66(8):5783-5793. doi:10.1002/pen.70609

BibTeX
@article{Tajari2026,
  author = {Tajari, Neda and Sadrnia, Hassan and Hosseini, Fereshteh and Ahmed, Jasim},
  title = {Fracture Behavior of Active PLA Food Packaging Films: EWF and SEM Analysis},
  journal = {Polymer Engineering & Science},
  year = {2026},
  volume = {66},
  number = {8},
  pages = {5783--5793},
  doi = {10.1002/pen.70609}
}
Start for free →