Microstructural Evolution and Differential Mechanical Degradation Mechanisms of GFRP Bars in Acidic and Alkaline Environments

Yunxia Wang, Xinghai Li, Chao Peng, Zhenghua Mao, Benxiang Tan, Tong Liu

Polymer Composites · 2026-11-17

DOI: 10.1002/pc.71876 ↗

At a glance

Journal article in Polymer Composites, published online on 2026-11-17. Written by Yunxia Wang and 5 co-authors. 50 references.

ΠερίληψηΒιβλιογραφικά στοιχείαCiteRelated studies

Abstract (original language)

Fiber‐reinforced polymer (FRP) composites may undergo mechanical degradation in aggressive chemical environments, while concentration‐dependent differences between acidic and alkaline exposure remain insufficiently characterized for the same GFRP bar system. In this study, pultruded vinyl‐ester GFRP bars were exposed at room temperature to H 2 SO 4 and NaOH solutions with concentrations ranging from 0.5 to 3.0 mol/L for 30 and 60 days. Density, tensile strength, and shear strength were evaluated, while SEM, qualitative EDS, and FTIR were used to characterize local material changes. Under H 2 SO 4 exposure, tensile‐strength retention remained at or above 97.0%, whereas shear‐strength retention decreased to 92.6% after 60 days in 3.0 mol/L solution. Localized fiber‐surface roughening and gaps near some fiber/resin boundaries were observed. Under NaOH exposure, tensile‐strength retention decreased to 90.0% under the same concentration and duration, while shear‐strength retention remained at 98.4%. More evident surface‐resin loss and fiber exposure were observed, and the FTIR results were consistent with alteration of the vinyl‐ester matrix. Thus, the same GFRP bar system exhibited a greater relative reduction in shear strength under H 2 SO 4 exposure but a greater relative reduction in tensile strength under NaOH exposure. An empirical semi‐logarithmic relationship was used to compare the apparent degradation rates only within the measured 0–60‐day interval. These results highlight the value of jointly assessing tensile and shear retention when characterizing the short‐term chemical durability of GFRP bars.

Cite

APA

Wang, Y., Li, X., Peng, C., Mao, Z., Tan, B., & Liu, T. (2026). Microstructural Evolution and Differential Mechanical Degradation Mechanisms of GFRP Bars in Acidic and Alkaline Environments. Polymer Composites. https://doi.org/10.1002/pc.71876

Vancouver

Wang Y, Li X, Peng C, Mao Z, Tan B, Liu T. Microstructural Evolution and Differential Mechanical Degradation Mechanisms of GFRP Bars in Acidic and Alkaline Environments. Polymer Composites. 2026. doi:10.1002/pc.71876

BibTeX
@article{Wang2026,
  author = {Wang, Yunxia and Li, Xinghai and Peng, Chao and Mao, Zhenghua and Tan, Benxiang and Liu, Tong},
  title = {Microstructural Evolution and Differential Mechanical Degradation Mechanisms of GFRP Bars in Acidic and Alkaline Environments},
  journal = {Polymer Composites},
  year = {2026},
  doi = {10.1002/pc.71876}
}
Start for free →