EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Surface Roughness and Wear Behavior of CAD/CAM Ceramics Against Vita Mark II

Amirhosein Habibnezhad, Gazaleh Ahmadi, Naeeme Naderi iD

Clinical and Experimental Dental Research · 2025

DOI: 10.1002/cre2.70174 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Clinical and Experimental Dental Research, 2025. Verfasst von Amirhosein Habibnezhad und 2 weiteren Autor:innen. Beteiligte Einrichtung: School of Dentistry, Babol University of Medical Sciences, Babol, Mazandaran Province, Iran. Hauptthemen laut MEDLINE: Computer-Aided Design, Ceramics, Dental Porcelain, Dental Restoration Wear. Die Arbeit nennt 40 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: This study was supported by the Babol University of Medical Sciences., Babol University of Medical Sciences.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Objectives

This study aimed to assess the surface roughness (SR) and wear behavior of computer‐aided design/computer‐aided manufacturing (CAD/CAM) ceramics when compared to a feldspathic ceramic. Material and Methods This in vitro study was conducted on three groups of CAD/CAM ceramic blocks ( n = 10 each): a zirconia‐reinforced lithium silicate ceramic, a polymer‐infiltrated ceramic network, and a resin nanoceramic. Additionally, 40 feldspathic ceramic blocks and 10 bovine incisors were used as antagonist materials. Surface roughness was measured by profilometry before and after wear testing (49 N, 120,000 cycles, 30 cycles/min). Wear depth was quantified using 3D scanning and image analysis software. Data were analyzed using ANOVA and paired t ‐tests (α = 0.05).

Results

Before wear testing, the zirconia‐reinforced ceramic showed significantly higher SR than the other groups ( p = 0.00). All groups exhibited a significant reduction in SR after testing ( p = 0.00). Posttest SR varied significantly between most groups ( p < 0.05), except between natural enamel and the resin nanoceramic ( p = 0.986). Wear depth differed significantly among the materials ( p < 0.001), with natural enamel showing the lowest wear, comparable only to the resin nanoceramic ( p > 0.05).

Conclusions

All tested CAD/CAM ceramics underwent substantial wear and SR reduction when opposed by feldspathic ceramic. The resin nanoceramic demonstrated the closest wear behavior to natural enamel and may be the most suitable restorative material for contact with feldspathic ceramics.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

Computer-Aided DesignCeramicsDental PorcelainDental Restoration WearSurface PropertiesAnimalsCattleZirconiumMaterials TestingAluminum SilicatesIn Vitro TechniquesPotassium Compounds

Stichwörter der Autor:innen

ceramicscomputer‐aided designdental restoration wearmechanical tests

Substanzen

Zirconiumzirconium oxideVita Mark IIDental PorcelainAluminum SilicatesfeldsparPotassium Compounds

Autor:innen und Institutionen

  • School of Dentistry, Babol University of Medical Sciences, Babol, Mazandaran Province, Iran.

ORCID-Profile: Naeeme Naderi

Förderung

  • This study was supported by the Babol University of Medical Sciences.
  • Babol University of Medical Sciences

Zitieren

APA

Habibnezhad, A., Ahmadi, G., & Naderi, N. (2025). Surface Roughness and Wear Behavior of CAD/CAM Ceramics Against Vita Mark II. Clinical and Experimental Dental Research. https://doi.org/10.1002/cre2.70174

Vancouver

Habibnezhad A, Ahmadi G, Naderi N. Surface Roughness and Wear Behavior of CAD/CAM Ceramics Against Vita Mark II. Clinical and Experimental Dental Research. 2025. doi:10.1002/cre2.70174

BibTeX
@article{Habibnezhad2025,
  author = {Habibnezhad, Amirhosein and Ahmadi, Gazaleh and Naderi, Naeeme},
  title = {Surface Roughness and Wear Behavior of CAD/CAM Ceramics Against Vita Mark II},
  journal = {Clinical and Experimental Dental Research},
  year = {2025},
  doi = {10.1002/cre2.70174}
}
Kostenlos starten →