Restraining Planar Gliding in Single‐Crystalline LiNi 0.9 Co 0.05 Mn 0.05 O 2 Cathodes by Combining Bulk and Surface Modification Strategies
Angewandte Chemie International Edition · 10.02.2025 · 64 (7)
DOI: 10.1002/anie.202419903 ↗Kurz gefasst
Fachartikel in der Zeitschrift Angewandte Chemie International Edition, online erschienen am 09.12.2024. Verfasst von Zhouliang Tan und 12 weiteren Autor:innen. Beteiligte Einrichtung: State Key Laboratory of Chemistry and Utilization of Carbon Based Energy Resources, College of Chemistry, Xinjiang University, Urumqi, Xinjiang, 8300…. Die Arbeit wurde bisher 32-mal zitiert (Crossref) und nennt 87 Literaturangaben. Gefördert von: National Natural Science Foundation of China, Key Project of Nature Science Foundation of Xinjiang Province, Major Projects of Xinjiang Province.
Abstract (Originalsprache)
The delamination cracking from planar gliding along the (003) facets and anisotropic lattice strain perpendicular to the (003) facets inevitable lead to degradation of Ni‐rich single‐crystal cathode materials, adversely affecting their cyclability. Herein, we rationally design a single‐crystal LiNi 0.9 Co 0.05 Mn 0.05 O 2 (SC90) cathode with robust chemo‐mechanical properties, in which coherently grown MgO 6 octahedra and BO 4 tetrahedra are incorporated into the lattice, and a stabilizing Mg 3 (BO 3 ) 2 layer is concurrently formed on the particle surface. Multiscale in /ex situ characterizations and theoretical calculations indicate that introducing the MgO 6 and BO 4 units leads to a “pinning effect” within the layered structure. This in turn strongly mitigates mechanical degradation by reducing planar gliding and delamination cracking over extended cycling. Moreover, the Mg 3 (BO 3 ) 2 coating maintains fast lithium diffusion by suppressing parasitic reactions at the cathode|electrolyte interface. The tailored SC90 cathode exhibits a capacity retention of ~88 % after 300 cycles at 5 C rate, significantly outperforming the pristine counterpart (~60 %). Additionally, a pouch‐type full cell with a graphite anode sustains a specific discharge capacity of 177 mAh g −1 after 500 cycles, with 90 % capacity retention. This work highlights the “pining effect” in preventing unfavorable slab sliding and structural deterioration, offering new insights for designing advanced ultrahigh Ni single‐crystal cathodes.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- State Key Laboratory of Chemistry and Utilization of Carbon Based Energy Resources, College of Chemistry, Xinjiang University, Urumqi, Xinjiang, 830017, China.
- State Key Lab for Physical Chemistry of Solid Surfaces & Department of Chemistry, College of Energy, Xiamen University, Xiamen, 361005, China.
- Institute of Nanotechnology, Karlsruhe Institute of Technology (KIT), Karlsruhe, 76131, Germany.
- School of Materials Science and Engineering, Zhengzhou University, Zhengzhou, 450001, China.
ORCID-Profile: Torsten Brezesinski, Yong Yang, Wengao Zhao
Förderung
- National Natural Science Foundation of China
- Key Project of Nature Science Foundation of Xinjiang Province
- Major Projects of Xinjiang Province
- Key Research and Development Project of Xinjiang Province
Zitieren
APA
Tan, Z., Chen, X., Lin, J., Huang, Y., Cheng, W., Liu, Q., Zhang, H., Ren, F., Huang, Y., Liu, Z., Brezesinski, T., Yang, Y., & Zhao, W. (2025). Restraining Planar Gliding in Single‐Crystalline LiNi 0.9 Co 0.05 Mn 0.05 O 2 Cathodes by Combining Bulk and Surface Modification Strategies. Angewandte Chemie International Edition, 64(7). https://doi.org/10.1002/anie.202419903
Vancouver
Tan Z, Chen X, Lin J, Huang Y, Cheng W, Liu Q, et al. Restraining Planar Gliding in Single‐Crystalline LiNi 0.9 Co 0.05 Mn 0.05 O 2 Cathodes by Combining Bulk and Surface Modification Strategies. Angewandte Chemie International Edition. 2025;64(7). doi:10.1002/anie.202419903
BibTeX
@article{Tan2025,
author = {Tan, Zhouliang and Chen, Xiaoxuan and Lin, Jing and Huang, Yudai and Cheng, Wenhua and Liu, Qingcui and Zhang, Han and Ren, Fucheng and Huang, Yingde and Liu, Zhenjie and Brezesinski, Torsten and Yang, Yong and Zhao, Wengao},
title = {Restraining Planar Gliding in Single‐Crystalline LiNi 0.9 Co 0.05 Mn 0.05 O 2 Cathodes by Combining Bulk and Surface Modification Strategies},
journal = {Angewandte Chemie International Edition},
year = {2025},
volume = {64},
number = {7},
doi = {10.1002/anie.202419903}
}
EUVIMED