Fachartikel in der Zeitschrift Advanced Materials, online erschienen am 13.02.2024. Verfasst von Yongsheng Ji und 11 weiteren Autor:innen. Beteiligte Einrichtung: State Key Laboratory of Material Processing and Die and Mold Technology, School of Materials Science and Engineering, Huazhong University of Science …. Die Arbeit wurde bisher 63-mal zitiert (Crossref) und nennt 77 Literaturangaben. Gefördert von: National Key R&D Program of China, Natural Science Foundation of Hubei Province, China, Interdisciplinary Research Program of Huazhong University of Science and Technology.
Abstract (Originalsprache)
Solid electrolyte interface (SEI) is arguably the most important concern in graphite anodes, which determines their achievable Coulombic efficiency (CE) and cycling stability. In spent graphite anodes, there are already‐formed (yet loose and/or broken) SEIs and some residual active lithium, which, if can be inherited in the regenerated electrodes, are highly desired to compensate for the lithium loss due to SEI formation. However, current graphite regenerated approaches easily destroy the thin SEIs and residue active lithium, making their reuse impossible. Herein, this work reports a fast‐heating strategy (e.g., 1900 K for ≈150 ms) to upcycle degraded graphite via instantly converting the loose original SEI layer (≈100 nm thick) to a compact and mostly inorganic one (≈10–30 nm thick with a 26X higher Young's Modulus) and still retaining the activity of residual lithium. Thanks to the robust SEI and enclosed active lithium, the regenerated graphite exhibited 104.7% initial CE for half‐cell and gifted the full cells with LiFePO 4 significantly improved initial CE (98.8% versus 83.2%) and energy density (309.4 versus 281.4 Wh kg −1 ), as compared with commercial graphite. The as‐proposed upcycling strategy turns the “waste” graphite into high‐value prelithiated ones, along with significant economic and environmental benefits.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- State Key Laboratory of Material Processing and Die and Mold Technology, School of Materials Science and Engineering, Huazhong University of Science and Technology, Wuhan, Hubei, 430074, China.
ORCID-Profile: Yonggang Yao
Förderung
- National Key R&D Program of China
- Natural Science Foundation of Hubei Province, China
- Interdisciplinary Research Program of Huazhong University of Science and Technology
- Fundamental Research Funds for the Central Universities
- National Key Research and Development Program of China
Zitieren
APA
Ji, Y., Zhang, H., Yang, D., Pan, Y., Zhu, Z., Qi, X., Pi, X., Du, W., Cheng, Z., Yao, Y., Qie, L., & Huang, Y. (2024). Regenerated Graphite Electrodes with Reconstructed Solid Electrolyte Interface and Enclosed Active Lithium Toward >100% Initial Coulombic Efficiency. Advanced Materials, 36(19). https://doi.org/10.1002/adma.202312548
Vancouver
Ji Y, Zhang H, Yang D, Pan Y, Zhu Z, Qi X, et al. Regenerated Graphite Electrodes with Reconstructed Solid Electrolyte Interface and Enclosed Active Lithium Toward >100% Initial Coulombic Efficiency. Advanced Materials. 2024;36(19). doi:10.1002/adma.202312548
BibTeX
@article{Ji2024,
author = {Ji, Yongsheng and Zhang, Hao and Yang, Dan and Pan, Yujun and Zhu, Zhenglu and Qi, Xiaoqun and Pi, Xinpeng and Du, Weichen and Cheng, Zhiheng and Yao, Yonggang and Qie, Long and Huang, Yunhui},
title = {Regenerated Graphite Electrodes with Reconstructed Solid Electrolyte Interface and Enclosed Active Lithium Toward >100% Initial Coulombic Efficiency},
journal = {Advanced Materials},
year = {2024},
volume = {36},
number = {19},
doi = {10.1002/adma.202312548}
}
EUVIMED