EUVIMEDEUVIMED entdecken
Crossref

Lithium Pre‐Storage Enables High Initial Coulombic Efficiency and Stable Lithium‐Enriched Silicon/Graphite Anode

Ying-Jie Gao, Cheng-Hao Cui, Zhi-Kun Huang, Guo-Yu Pan, Yuan-Fan Gu, Ya-Nan Yang, Fan Bai, Zhuang Sun, Tao Zhang iD

Angewandte Chemie International Edition · 2024-07 · 63 (27)

DOI: 10.1002/anie.202404637 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Angewandte Chemie International Edition, online erschienen am 28.05.2024. Verfasst von Ying-Jie Gao und 8 weiteren Autor:innen. Beteiligte Einrichtung: State Key Lab of High Performance Ceramics and Superfine microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Dingxi Roa…. Die Arbeit wurde bisher 45-mal zitiert (Crossref) und nennt 51 Literaturangaben. Gefördert von: National Natural Science Foundation of China.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Application of silicon‐based anodes is significantly challenged by low initial Coulombic efficiency (ICE) and poor cyclability. Traditional pre‐lithiation reagents often pose safety concerns due to their unstable chemical nature. Achieving a balance between water‐stability and high ICE in prelithiated silicon is a critical issue. Here, we present a lithium‐enriched silicon/graphite material with an ultra‐high ICE of ≥110 % through a high‐stable lithium pre‐storage methodology. Lithium pre‐storage prepared a nano‐drilled graphite material with surficial lithium functional groups, which can form chemical bonds with adjacent silicon during high‐temperature sintering. This results in an unexpected O−Li−Si interaction, leading to in situ pre‐lithiation of silicon nanoparticles and providing high stability in air and water. Additionally, the lithium‐enriched silicon/graphite materials impart a combination of high ICE, high specific capacity (620 mAh g −1 ), and long cycling stability (>400 cycles). This study opens up a promising avenue for highly air‐ and water‐stable silicon anode prelithiation methods.

Schlagwörter

Stichwörter der Autor:innen

Lithium pre-storagehigh initial Coulombic efficiencylithium-enriched silicon/graphite materialpre-lithiationsilicon-based anode

Autor:innen und Institutionen

  • State Key Lab of High Performance Ceramics and Superfine microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Dingxi Road, Shanghai, 200050, P. R. China.
  • Center of Materials Science and Optoelectronics Engineering, University of Chinese Academy of Sciences, Beijing, 100049, P. R. China.
  • CAS Key Laboratory of Materials for Energy Conversion Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Dingxi Road, Shanghai, 200050, P. R. China.

ORCID-Profile: Tao Zhang

Förderung

  • National Natural Science Foundation of China

Zitieren

APA

Gao, Y. J., Cui, C. H., Huang, Z. K., Pan, G. Y., Gu, Y. F., Yang, Y. N., Bai, F., Sun, Z., & Zhang, T. (2024). Lithium Pre‐Storage Enables High Initial Coulombic Efficiency and Stable Lithium‐Enriched Silicon/Graphite Anode. Angewandte Chemie International Edition, 63(27). https://doi.org/10.1002/anie.202404637

Vancouver

Gao YJ, Cui CH, Huang ZK, Pan GY, Gu YF, Yang YN, et al. Lithium Pre‐Storage Enables High Initial Coulombic Efficiency and Stable Lithium‐Enriched Silicon/Graphite Anode. Angewandte Chemie International Edition. 2024;63(27). doi:10.1002/anie.202404637

BibTeX
@article{Gao2024,
  author = {Gao, Ying-Jie and Cui, Cheng-Hao and Huang, Zhi-Kun and Pan, Guo-Yu and Gu, Yuan-Fan and Yang, Ya-Nan and Bai, Fan and Sun, Zhuang and Zhang, Tao},
  title = {Lithium Pre‐Storage Enables High Initial Coulombic Efficiency and Stable Lithium‐Enriched Silicon/Graphite Anode},
  journal = {Angewandte Chemie International Edition},
  year = {2024},
  volume = {63},
  number = {27},
  doi = {10.1002/anie.202404637}
}
Kostenlos starten →