Fracture Resistance of Endodontically Treated Premolars Reinforced with Two Different Fibers -A Comparative In Vitro Evaluation

Veena S pai, Ajay Kumar D G

IOSR Journal of Dental and Medical Sciences · 2026-08 · 25 (8) · 46-54

DOI: 10.9790/0853-2508044654 ↗

Kurz gefasst

Fachartikel in der Zeitschrift IOSR Journal of Dental and Medical Sciences, 2026-08. Verfasst von Veena S pai und 1 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Background

Endodontically treated teeth are structurally weakened due to loss of tooth structure during endodontic procedures. Premolars are highly susceptible to fracture because of thin cuspal walls and reduced cervical dimensions, leading to cuspal deflection under occlusal forces. Composite resin restorations provide bonding but may not fully restore fracture resistance due to polymerization shrinkage and limited toughness. Fiber reinforced composites improve stress distribution and prevent crack propagation. This study aimed to evaluate and compare fracture resistance of endodontically treated premolars reinforced with polyethylene fibers and ultrathin glass fiber strips. Materials and Methods: Sixty extracted mandibular first premolars were randomly divided into three groups (n = 20). Group I received composite resin, Group II polyethylene fiber reinforced composite, and Group III ultrathin glass fiber strip reinforced composite. Standardized root canal treatment and cavity preparation were performed. Fracture resistance was tested using a universal testing machine, and fracture load was recorded in Newtons. Data were analysed using one-way ANOVA and Tukey’s post hoc test.

Results

Mean fracture resistance values were 855.15 ± 10.15 N (Group I), 899.90 ±7.25 N (Group II), and 916.75 ± 6.18 N (Group III). A statistically significant difference was observed (p < 0.001). Group III showed highest fracture resistance followed by Group II and Group I.

Conclusion

Fiber reinforcement significantly improved fracture resistance compared to composite alone. Ultrathin glass fiber strips demonstrated superior performance over polyethylene fibers. This indicates that fiber reinforcement, especially ultrathin glass fiber strips, is an effective conservative approach to enhance fracture resistance of endodontically treated premolars

Zitieren

APA

pai, V. S., & G, A. K. D. (2026). Fracture Resistance of Endodontically Treated Premolars Reinforced with Two Different Fibers -A Comparative In Vitro Evaluation. IOSR Journal of Dental and Medical Sciences, 25(8), 46-54. https://doi.org/10.9790/0853-2508044654

Vancouver

pai VS, G AKD. Fracture Resistance of Endodontically Treated Premolars Reinforced with Two Different Fibers -A Comparative In Vitro Evaluation. IOSR Journal of Dental and Medical Sciences. 2026;25(8):46-54. doi:10.9790/0853-2508044654

BibTeX
@article{pai2026,
  author = {pai, Veena S and G, Ajay Kumar D},
  title = {Fracture Resistance of Endodontically Treated Premolars Reinforced with Two Different Fibers -A Comparative In Vitro Evaluation},
  journal = {IOSR Journal of Dental and Medical Sciences},
  year = {2026},
  volume = {25},
  number = {8},
  pages = {46--54},
  doi = {10.9790/0853-2508044654}
}
Kostenlos starten →