Effect of calcium hydroxide removal protocols on push-out bond strength of hydraulic calcium silicate sealers: an in vitro study
PeerJ · 14.05.2026 · 14 · e21236
DOI: 10.7717/peerj.21236 ↗Kurz gefasst
Fachartikel in der Zeitschrift PeerJ, online erschienen am 14.05.2026. Verfasst von Özlem Sivas Yılmaz und 2 weiteren Autor:innen. Beteiligte Einrichtung: Department of Endodontics, Faculty of Dentistry, Abant Izzet Baysal University, Bolu, Turkey. Hauptthemen laut MEDLINE: Silicates, Calcium Hydroxide, Calcium Compounds, Root Canal Filling Materials. Die Arbeit nennt 34 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
Background and Objectives This study aims to evaluate the push-out bond strength of a hydraulic calcium silicate sealer (HCSS) (AH Plus Bioceramic; Dentsply Sirona, Tulsa, OK, USA), to dentin following calcium hydroxide (Ca(OH) 2 ) removal using different irrigation protocols and to assess the sealer-dentin adhesive interface. Materials and Methods Forty-four single-rooted human teeth were prepared, standardized to 16 mm in length, and instrumented with ProTaper Next to an X5 size. After final irrigation, the canals were filled with Ca(OH) 2 for two weeks. The specimens were divided into four groups according to the irrigation protocol: distilled water (control), ethylenediaminetetraacetic acid (EDTA) combined with NaOCl, citric acid, and glycolic acid. The canals were subsequently dried and filled with HCSS, a premixed hydraulic calcium silicate sealer, using an X5 gutta-percha cone. The specimens were stored at 37 °C and 100% humidity for 7-day before testing. Push-out bond strength was measured using a universal testing machine, and failure modes were evaluated under a stereomicroscope.
Results
Glycolic acid exhibited the highest overall bond strength, particularly in the coronal third ( p < .05), compared to distilled water. EDTA + NaOCl and citric acid demonstrated similar bond strength values, both statistically superior to distilled water ( p < .05), but not significantly different from glycolic acid ( p > .05). Failure mode analysis revealed predominantly cohesive failures, with no statistically significant variation in failure modes among irrigation protocols or root canal thirds ( p > .05).
Conclusion
The irrigation protocol used for Ca(OH) 2 removal significantly influenced the push-out bond strength of HCSS. Glycolic acid demonstrated the highest bond strength, particularly in the coronal third, while EDTA + NaOCl and citric acid also enhanced bonding compared to the control group.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Department of Endodontics, Faculty of Dentistry, Abant Izzet Baysal University, Bolu, Turkey.
- Department of Endodontics, Faculty of Dentistry, Ondokuz Mayis University Samsun, Turkey.
Zitieren
APA
Sivas Yılmaz, Ö., Keskin, C., & Güven Kömürcü, A. (2026). Effect of calcium hydroxide removal protocols on push-out bond strength of hydraulic calcium silicate sealers: an in vitro study. PeerJ, 14, e21236. https://doi.org/10.7717/peerj.21236
Vancouver
Sivas Yılmaz Ö, Keskin C, Güven Kömürcü A. Effect of calcium hydroxide removal protocols on push-out bond strength of hydraulic calcium silicate sealers: an in vitro study. PeerJ. 2026;14:e21236. doi:10.7717/peerj.21236
BibTeX
@article{SivasYlmaz2026,
author = {Sivas Yılmaz, Özlem and Keskin, Cangül and Güven Kömürcü, Ayşegül},
title = {Effect of calcium hydroxide removal protocols on push-out bond strength of hydraulic calcium silicate sealers: an in vitro study},
journal = {PeerJ},
year = {2026},
volume = {14},
pages = {e21236},
doi = {10.7717/peerj.21236}
}
EUVIMED