A Comparative Evaluation of Dimensional Stability and Accuracy of Zinc Oxide Eugenol Paste and Modelling Wax as Interocclusal Recording Materials. An In Vitro Study

Shahnaj Begum, Md Shafiqul Islam, Md Mostafijur Rahman, Chowdhury Afrina Parvin, Arzu Akter, Israt Jahan, Khyrun Nahar, Shahidul Islam Fuad

Naogaon Medical College Journal · 10.11.2026 · 3 (2) · 35-40

DOI: 10.70818/nmcj.v03i02.073 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Naogaon Medical College Journal, online erschienen am 10.11.2026. Verfasst von Shahnaj Begum und 7 weiteren Autor:innen. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Background

Accurate interocclusal records are essential for the successful fabrication of indirect dental prostheses. Dimensional stability of the recording material plays a critical role in maintaining the accuracy of maxillomandibular relationships. Among the commonly used interocclusal recording materials, Zinc Oxide Eugenol (ZOE) paste and modelling wax continue to be widely employed because of their availability and ease of manipulation.

Objective

To compare the dimensional stability and accuracy of Zinc Oxide Eugenol paste and modelling wax as interocclusal recording materials at different time intervals.

Methods

This comparative in vitro study was conducted in the Department of Prosthodontics, Faculty of Dentistry, BSMMU, Dhaka from June 2009 to June 2010. Forty duplicated disks were prepared from a custom-made stainless-steel die. Ten specimens each were fabricated using polyvinyl siloxane, ZOE paste, alginate and modelling wax. For the present comparison, data from Group B (ZOE paste) and Group D (modelling wax) were analyzed. Horizontal linear distances between reference lines A and C were measured using a travelling micrometer microscope at 1 hour, 24 hours, 48 hours and 72 hours.

Results

Both ZOE paste and modelling wax demonstrated progressive dimensional changes over time. In Group B, mean horizontal distance decreased from 5.81±0.06 mm at 1 hour to 5.51±0.07 mm at 72 hours. In Group D, the corresponding values decreased from 5.69±0.08 mm to 5.47±0.03 mm. All intragroup comparisons showed statistically significant dimensional changes (p

Zitieren

APA

Begum, S., Islam, M. S., Rahman, M. M., Parvin, C. A., Akter, A., Jahan, I., Nahar, K., & Fuad, S. I. (2026). A Comparative Evaluation of Dimensional Stability and Accuracy of Zinc Oxide Eugenol Paste and Modelling Wax as Interocclusal Recording Materials. An In Vitro Study. Naogaon Medical College Journal, 3(2), 35-40. https://doi.org/10.70818/nmcj.v03i02.073

Vancouver

Begum S, Islam MS, Rahman MM, Parvin CA, Akter A, Jahan I, et al. A Comparative Evaluation of Dimensional Stability and Accuracy of Zinc Oxide Eugenol Paste and Modelling Wax as Interocclusal Recording Materials. An In Vitro Study. Naogaon Medical College Journal. 2026;3(2):35-40. doi:10.70818/nmcj.v03i02.073

BibTeX
@article{Begum2026,
  author = {Begum, Shahnaj and Islam, Md Shafiqul and Rahman, Md Mostafijur and Parvin, Chowdhury Afrina and Akter, Arzu and Jahan, Israt and Nahar, Khyrun and Fuad, Shahidul Islam},
  title = {A Comparative Evaluation of Dimensional Stability and Accuracy of Zinc Oxide Eugenol Paste and Modelling Wax as Interocclusal Recording Materials. An In Vitro Study},
  journal = {Naogaon Medical College Journal},
  year = {2026},
  volume = {3},
  number = {2},
  pages = {35--40},
  doi = {10.70818/nmcj.v03i02.073}
}
Kostenlos starten →