EUVIMEDEUVIMED entdecken
Crossref

Radiographic Evaluation of Welding Defects in Natural Gas Pipeline Joints. Part 2: Film Radiography of Large-Diameter (16″) API X65 Spiral SAW Pipe Welds

Ghadah Sheemah

South Mediterranean University Journal of Pure and Applied Sciences · 2026

DOI: 10.67525/rgd3yg55 ↗

Kurz gefasst

Fachartikel in der Zeitschrift South Mediterranean University Journal of Pure and Applied Sciences, 2026. Verfasst von Ghadah Sheemah.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study evaluates the integrity and quality of large-diameter natural gas transmission pipeline welded joints using film radiography with gamma-ray (Ir-192) and X-ray sources. Three 16″ diameter API X65 spiral submerged arc welded (SAW) pipe specimens were examined using panoramic single-exposure and doublewall single-image techniques in accordance with EN 1435, allowing a direct comparison between gamma-ray and X-ray detection of the same defect categories at equivalent wall thickness. The resulting radiographic films were evaluated against the acceptance criteria of API 1104 and ASME Section V. Insufficient melting, incomplete filling, outer combustion groove, concavity, burn-and-drill, and single- and double-sided cold lap indications were identified and classified by density, length, and position. Insufficient melting, burn-and-drill, and cold lap defects exceeded the length limits of API 1104 Section 8 and required repair by grinding, while outer combustion groove and root concavity remained within acceptance limits. Unlike the small-diameter specimens examined in Part 1, where defects traced to root-pass control by a single welder, defects in this large-diameter spiral SAW group traced to the automated multi-head submerged arc process and to joint-bevel contamination, confirming welding process, rather than pipe diameter, as the stronger predictor of defect type. Gamma-ray and X-ray exposures of comparable defect types produced consistent classification outcomes against API 1104, indicating that source selection did not materially affect defect detectability at the wall thicknesses examined. The results confirm that panoramic and double-wall exposure geometries remain reliable for detecting and classifying welding defects in large-diameter spiral SAW pipeline girth welds

Zitieren

APA

Sheemah, G. (2026). Radiographic Evaluation of Welding Defects in Natural Gas Pipeline Joints. Part 2: Film Radiography of Large-Diameter (16″) API X65 Spiral SAW Pipe Welds. South Mediterranean University Journal of Pure and Applied Sciences. https://doi.org/10.67525/rgd3yg55

Vancouver

Sheemah G. Radiographic Evaluation of Welding Defects in Natural Gas Pipeline Joints. Part 2: Film Radiography of Large-Diameter (16″) API X65 Spiral SAW Pipe Welds. South Mediterranean University Journal of Pure and Applied Sciences. 2026. doi:10.67525/rgd3yg55

BibTeX
@article{Sheemah2026,
  author = {Sheemah, Ghadah},
  title = {Radiographic Evaluation of Welding Defects in Natural Gas Pipeline Joints. Part 2: Film Radiography of Large-Diameter (16″) API X65 Spiral SAW Pipe Welds},
  journal = {South Mediterranean University Journal of Pure and Applied Sciences},
  year = {2026},
  doi = {10.67525/rgd3yg55}
}
Kostenlos starten →