Effect of Firing Temperature on the Microstructural Characteristics of Nickel Chromium Alloy–Porcelain Interface: An In Vitro Scanning Electron Microscopy Study
Bangladesh Journal of Dental Research & Education · 01.07.2026 · 16 (2) · 34
DOI: 10.67201/bjdre.v16i2.155 ↗Kurz gefasst
Fachartikel in der Zeitschrift Bangladesh Journal of Dental Research & Education, online erschienen am 01.07.2026. Verfasst von Noor Akhter Hafiza und 3 weiteren Autor:innen. Die Arbeit nennt 17 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
Background
The alloy-ceramic interface influences the long-term success of porcelain-fused-to-metal restorations. The tension at interface can accomplish if there is no alteration in microstructure. The firing temperature's impact on the nickel-chromium alloy–porcelain interface's microstructural characteristics was assessed using a scanning electron microscope (SEM). Materials and methods: According to ADA specifications, 56 strips of porcelain-veneered nickel-chromium alloy were prepared to form 20 × 5 × 3 mm. They were placed in two groups: 28 samples were made 900 °C hot and 28 samples were made 960 °C hot. All the samples were subjected to SEM at 800× magnification for assessment of interface irregularities at the metal-ceramic junction. Using a standardized 4-point scoring system (0–3), interface irregularities were scored. Mann–Whitney U test was performed for statistical analysis.
Results
At 960°C, the samples were found to have a significantly lower irregularities at the interface when compared to 900°C (mean rank 21.91 900°C shows 35.09, p = 0.00252). At a temperature of 900 °C, around 15 samples demonstrated 3 – 4 interface irregularities, whereas at 960 °C, only 6 samples exhibited such level of irregularity. The difference was statistically significant as shown by the Mann-Whitney U test (U = 207.5, Z = 3.0152, p = 0.00252).
Conclusion
The microstructure of metal-porcelain bonding interface is influenced by firing temperature. When fired at 960°C, the metal/ceramic interface was found to be largely free of imperfections. This inference implies that firing at this temperature enhances bonding, thereby resulting in improved clinical performance of the metal-ceramic restoration.
Zitieren
APA
Hafiza, N. A., Rahman, M. M., Rahman, A. A., & Anjum, A. (2026). Effect of Firing Temperature on the Microstructural Characteristics of Nickel Chromium Alloy–Porcelain Interface: An In Vitro Scanning Electron Microscopy Study. Bangladesh Journal of Dental Research & Education, 16(2), 34. https://doi.org/10.67201/bjdre.v16i2.155
Vancouver
Hafiza NA, Rahman MM, Rahman AA, Anjum A. Effect of Firing Temperature on the Microstructural Characteristics of Nickel Chromium Alloy–Porcelain Interface: An In Vitro Scanning Electron Microscopy Study. Bangladesh Journal of Dental Research & Education. 2026;16(2):34. doi:10.67201/bjdre.v16i2.155
BibTeX
@article{Hafiza2026,
author = {Hafiza, Noor Akhter and Rahman, Md. Mahbubur and Rahman, AKM Anisur and Anjum, Atia},
title = {Effect of Firing Temperature on the Microstructural Characteristics of Nickel Chromium Alloy–Porcelain Interface: An In Vitro Scanning Electron Microscopy Study},
journal = {Bangladesh Journal of Dental Research & Education},
year = {2026},
volume = {16},
number = {2},
pages = {34},
doi = {10.67201/bjdre.v16i2.155}
}
EUVIMED