Balancing Nickel Recovery, Iron Dissolution, Acid Dosage, and Residence Time in Atmospheric Sulfuric Acid Leaching of a Ferruginous Lateritic Nickel Ore

Antonio Clareti Pereira

Journal International Review of Research Studies · 07.07.2026 · 1 (09) · 1-30

DOI: 10.66104/dempc459 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal International Review of Research Studies, online erschienen am 07.07.2026. Verfasst von Antonio Clareti Pereira. Die Arbeit wurde bisher 3-mal zitiert (Crossref). Der Volltext ist frei zugänglich (Open Access, CC BY-NC 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Atmospheric sulfuric acid leaching of ferruginous lateritic nickel ores requires a compromise between nickel recovery, iron dissolution, acid dosage, and residence time. In this study, a limonitic nickel ore fraction retained at 100 mesh was leached at approximately 95-100 °C using 700-1000 kg H₂SO₄/t ore while maintaining a constant initial slurry mass and solid-liquid basis. The ore contained approximately 1.08 wt.% Ni and 33.53 wt.% Fe, and mineralogical characterization indicated that nickel was mainly associated with iron oxyhydroxides, Si-Fe plasma, and subordinate phyllosilicates. Corrected extraction values showed that nickel extraction increased with acid dosage and residence time, reaching 84.9% at 700 kg/t and 420 min, 89.3% at 800 kg/t and 420 min, and 91.0% at 900 kg/t and 420 min. However, iron dissolution also increased, particularly at higher acid dosages. The 1000 kg/t condition was retained from 240 to 420 min after recalculation by direct liquid-wash-residue mass balance; it reached 83.1-89.5% Ni but dissolved 71.3-80.4% Fe, indicating severe loss of selectivity. Apparent pseudo-first-order and shrinking-core-type models were used as diagnostic tools, not as definitive mechanistic proof. A process-oriented acid-Fe-time penalty index was developed to rank feasible operating conditions. The selected practical compromise was 800 kg H₂SO₄/t ore and 300 min, achieving 82.8% Ni extraction with 48.4% Fe dissolution while avoiding the higher acid and residence-time penalties associated with more aggressive conditions.

Zitieren

APA

Pereira, A. C. (2026). Balancing Nickel Recovery, Iron Dissolution, Acid Dosage, and Residence Time in Atmospheric Sulfuric Acid Leaching of a Ferruginous Lateritic Nickel Ore. Journal International Review of Research Studies, 1(09), 1-30. https://doi.org/10.66104/dempc459

Vancouver

Pereira AC. Balancing Nickel Recovery, Iron Dissolution, Acid Dosage, and Residence Time in Atmospheric Sulfuric Acid Leaching of a Ferruginous Lateritic Nickel Ore. Journal International Review of Research Studies. 2026;1(09):1-30. doi:10.66104/dempc459

BibTeX
@article{Pereira2026,
  author = {Pereira, Antonio Clareti},
  title = {Balancing Nickel Recovery, Iron Dissolution, Acid Dosage, and Residence Time in Atmospheric Sulfuric Acid Leaching of a Ferruginous Lateritic Nickel Ore},
  journal = {Journal International Review of Research Studies},
  year = {2026},
  volume = {1},
  number = {09},
  pages = {1--30},
  doi = {10.66104/dempc459}
}
Kostenlos starten →